HEDP、PBTCA、Zn^(2+)复配对黄河恶化水中316L、317L的缓蚀阻垢作用 被引量:4

Corrosion and scale inhibition effect of complexes of HEDP,PBTCA and Zn^(2+) on 316L and 317L in deteriorated Yellow River water
下载PDF
导出
摘要 针对黄河水质恶化且波动大的问题,研究了HEDP、PBTCA、Zn2+复配对凝汽器管材316L、317L在黄河恶化水质中的缓蚀阻垢效果。结果表明,加入该复配缓蚀剂后:材质316L、317L在黄河恶化水质中的腐蚀电流明显减小;316L、317L阻抗谱呈现出2个容抗弧特征,阴极过程存在2种阴极反应且受活化控制,同时一部分结垢产物形貌由薄片状向球状及棒状转变。表明HEDP、PBTCA、Zn2+复配对316L、317L在黄河恶化水中的缓蚀阻垢效果显著。 The problems like water quality deterioration and fluctuation occurred in Yellow River become more and more severe.Therefore,the complex solution containing HEDP,PBTCA and Zn2+with a certain concentration was developed and used as inhibitor for condenser tube material(316Land 317Lsteel)in deteriorated Yellow River water.The polarization curves show that,the corrosion currents of 316 Land 317L in the deteriorated water decreased obviously.The electrochemical impedance spectroscopy(EIS)test results imply that,two capacitive impedance arcs appeared in the EIS of 316 Land 317L,indicating there were two cathode reactions controlled by active process.Some of the morphologies of scaling products on surface of 316 Land 317Lchanged from flake film to spheroid and rod like.
出处 《热力发电》 CAS 北大核心 2014年第8期111-115,共5页 Thermal Power Generation
关键词 凝汽器 316L 317L 复配缓蚀剂 缓蚀阻垢 交流阻抗 极化曲线 316L 317L corrosion and scale inhibitor EIS polarization curve
  • 相关文献

参考文献11

二级参考文献61

共引文献132

同被引文献43

引证文献4

二级引证文献9

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部