工业管道应力腐蚀裂纹的检验 被引量:5

Inspection of Stress Corrosion Crack Occurred in Industrial Piping
下载PDF
导出
摘要 概述了金属材料应力腐蚀裂纹的特点,提出了工业管道对其检验的内容和方法,通过对应力腐蚀裂纹宏观和微观特征的检查和分析,基本可以区别应力腐蚀裂纹和其他裂纹。应力腐蚀裂纹是比较危险的缺陷,因此在管道检修和设计时应采取必要的改进措施,防患于未然。 The features of stress corrosion crack appeared in metal were briefly described in this article. Stress corrosion crack is relative dangerous defect. With the examination and analysis of macro and micro features in stress corrosion crack, it can be separated from other cracks, so that the inspection method for stress corrosion crack was proposed.
作者 王建运
出处 《化工设备与管道》 CAS 2011年第3期62-64,共3页 Process Equipment & Piping
关键词 工业管道 应力腐蚀裂纹 检验及预防措施 industrial piping stress corrosion crack inspection and protection measure
  • 相关文献

参考文献5

二级参考文献4

共引文献14

同被引文献27

  • 1安玉龙 黎圣藜.安全阀的计算和选用.石油化工设计,1993,10(3):54-65. 被引量:1
  • 2Chen S H,Yeh R T,Cheng T P,et al.Hydrogen Sul-phide Stress Corrosion Cracking of TIG and LaserWelded 304 Stainless Steel[J].Corrosion Science,1994,36(12):2029-2041. 被引量:1
  • 3ASTM A240—1997,Standard Specification for Heat-Resisting Chromum and Chromium-Nickel StainlessSteel Plate,Sheet,and Strip for Pressure Vessels[S]. 被引量:1
  • 4ASTM-E140—2007,Standard Hardness Conversion Tablesfor Metals Relationship Among Brinell Hardness,VickersHardness,Rockwell Hardness,Superficial Hardness,Knoop Hardness,and Scleroscope Hardness[S]. 被引量:1
  • 5NACE MR0175—2002,Sulfide Stress Cracking Resist-ant Metallic Materials for Oilfield Equipment 3.5P10-13 2002[S]. 被引量:1
  • 6GB/T1467-1978,冶金产品化学分析方法标准的总则及一般规定[S]. 被引量:1
  • 7GB6654-86,压力容器用钢板[s]. 被引量:1
  • 8GB150一1998,钢制压力窖器[s]. 被引量:1
  • 9曾志果,林铁,康媞.污水中硫化氢的危害及其治理方法[J].广西轻工业,2008,24(3):89-90. 被引量:14
  • 10肖建军.CF-62钢制球罐硫化氢应力腐蚀裂纹分析及处理[J].岳阳职业技术学院学报,2008,23(5):85-89. 被引量:1

引证文献5

二级引证文献9

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部