摘要 以铅锌尾矿为主要原料,掺入石膏、石粉、水泥制备免烧砖,考察了各组分含量和用水量对免烧砖性能影响。结果显示,较佳成型水分为14%,成型压力为20 MPa,尾矿∶石膏∶水泥∶石粉=2.5∶1.5∶1∶5时,制备的免烧砖满足《非烧结垃圾尾矿砖》MU25级别要求,固废使用量达到25%,实现了固体废弃物的资源化。 Using tailings,gypsum,cement and stone powder to prepare the no-fire brick,the mechanical properties are discussed by change of the proportion of tailings、gypsum、cement and stone powder,and the dosage of the water.The results show that the best preparation condition is that the proportion of tailings、gypsum、cement and stone powder being 2.5∶1.5∶1∶5,the water consumption accounting for 14%of the total solid materials.The prepared non-fired bricks can meet the standard requirements of iron tailings,the use of solid waste reached 25%,realizing the recycling of solid waste.
作者 周龙 周素莲 马华菊 Zhou Long;Zhou Sulian;Ma Huaju(Guilin University of Technology at Nanning,Nanning,Guangxi,China)
出处 《矿产综合利用》 CAS 北大核心 2022年第3期12-16,共5页 Multipurpose Utilization of Mineral Resources
基金 广西科技基地与人才专项(桂科AD17129007)。
关键词 组分比例 用水量 免烧砖 抗压强度 吸水率 Component ratio Water consumption Non-fired brick Compressive strength Water absorption
  • 相关文献

参考文献11

二级参考文献106

共引文献88

同被引文献220

引证文献9

二级引证文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部