摘要
针对广西某低品位铜镍硫化矿石性质特点,采用铜镍混合浮选—抑镍浮铜工艺流程对该矿石进行了开发利用工艺技术条件研究。结果表明:以草酸为铜镍混浮的活化剂,活性炭为铜镍分离的脱药剂,石灰、亚硫酸钠和SY为铜镍分离时镍的组合抑制剂,采用1粗4扫铜镍混合浮选、1粗2精2扫铜镍分离、中矿顺序返回流程处理该矿石,最终获得了铜品位为15.24%、铜回收率为76.65%的铜精矿,以及镍品位为4.90%、镍回收率为82.36%的镍精矿。
Aiming at the characteristics of a low-grade copper and nickel sulfide ore in Guangxi, development and uti- lization of the ore were carried out by the process of Cu-Ni bulk flotation-copper floating and nickel inhibiting. The results showed that with oxalate as activator of Cu-Ni bulk flotation, activated carbon as reagent removal for separation of Copper and Nickel, the lime, sodium sulphite and SY as the combining depressant for separation of copper and nickel, copper con- centrate with Cu grade of 15.24% and recovery of 76.65%, and nickel concentrate with Ni grade of 4.90% and recovery of 82.36% were obtained by adopting the process of one roughing and four scavenging for Cu-Ni bulk flotation, one roug- hing, two cleaning and two scavenging for separation copper and nickel, and middles back to the flowsheet in turn.
出处
《金属矿山》
CAS
北大核心
2013年第9期84-87,共4页
Metal Mine
关键词
硫化铜镍矿
混合浮选
活性炭脱药
组合抑制剂
Copper-nickel sulfide ore, Bulk flotation, Reagent removal with activated carbon, Combining depressants