0Cr18Ni10Ti换热器热处理后产生裂纹原因分析及改进措施 被引量:2

CAUSE ANALYSIS ON THE CRACK FROM HEAT TREATMENT IN THE 0CR18NI10TI HEAT EXCHANGER AND THE IMPROVING MEASURES
下载PDF
导出
摘要 0Cr18Ni10Ti奥氏体不锈钢一般情况下具有良好的焊接性能,但由于其组织和成分的特殊性使其在某些操作条件下,会在焊接部位产生裂纹。文章分析了0Cr18Ni10Ti奥氏体不锈钢换热器在稳定化热处理后产生裂纹的原因,提出了有针对性的改进措施,为解决0Cr18Ni10Ti奥氏体不锈钢在热处理后出现裂纹的问题提供了一定的参考依据。 0Cr18Ni10Ti austenitic stainless steel usually has good welding performance,but because of its particular structure and component,crack generates in welding area under some working conditions.This paper analyzes the causes for the crack from stabilizing heat treatment in the 0Cr18Ni10Ti austenitic stainless steel heat exchanger.It puts forward some pertinent improving measures,which provides reference for solving the crack problem of the 0Cr18Ni10Ti austenitic stainless steel caused by heat treatment.
作者 林罡明
出处 《石油化工设备技术》 CAS 2012年第4期61-63,72,共3页 Petrochemical Equipment Technology
关键词 0Cr18Ni10Ti奥氏体不锈钢 稳定化热处理 裂纹 改进措施 0Cr18Ni10Ti austenitic stainless steel Stabilizing heat treatment Crack Improving measures
  • 相关文献

参考文献4

二级参考文献2

  • 1英若采.熔焊原理及金属材料焊接(第2版).北京:机械工业出版社.2004. 被引量:2
  • 2中国机械工程学会焊接学会编.焊接手册[M].北京:机械工业出版社,2003-04. 被引量:3

共引文献10

同被引文献7

引证文献2

二级引证文献5

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部