摘要
采用乙二胺四乙酸二酐(EDTAD)和醛基封端聚乙二醇(PEG-dial)对明胶蛋白进行酰化及还原胺化改性,然后与戊二醛(GTA)交联制备了复合改性明胶蛋白凝胶。研究了EDTAD、PEG-dial、交联剂等的用量对凝胶性能的影响,结果表明,随EDTAD用量的增多及GTA用量的减少凝胶的平衡溶胀率增大,PEG-dial的引入提高了破裂强度,所得凝胶的溶胀率为160g/g,破裂强度为16g。采用IR和SEM对其进行结构表征,结果表明,改性后明胶蛋白上引入了羧基和长碳链,复合改性后凝胶的微观结构更有序。
A EDTAD-PEG-dial-gelatin compound modified gel is prepared firstly by acylating gelatin protein with ethylenediaminetetraacetic dianhydride(EDTAD), followed by reducing amination with PEG-dial, and then by cross-linking with glutaraldehyde. The effects of the amount of EDTAD, PEG-dial and glutaraldehyde(GTA) on the properties of gelatin gel are discussed. The results show that the swelling ratio of gels increases with increasing amount of EDTAD or decreasing amount of GTA. The rupture strength of gels is improved by introducing PEG-dial into gelatin molecules. The swelling ratio and rupture strength of gels are 160g/g and 16g respectively. The acylated ge- latin protein is characterized by IR and the gel is characterized by SEM, it is found that more hydrophilic carboxyl group and long carbon chain of PEG are introduced into gelatin molecules, and a more ordered structure is obtained by compound modifying.
出处
《材料导报》
EI
CAS
CSCD
北大核心
2010年第4期41-44,共4页
Materials Reports
基金
广东省绿色化学产品技术重点实验室开放基金(GC200702)
广东工业大学博士启动基金课题(063027)
关键词
明胶凝胶
酰化
还原胺化
溶胀率
破裂强度
gelatin gel, acylation, reductive amination, swelling ratio, rupture strength