骨胶对建筑石膏水化和硬化体微结构的影响 被引量:9

Influence of Macromolecule-type Retarders on the Hydration and Microstructure of Hardened Paste
下载PDF
导出
摘要 研究了大分子类缓凝剂骨胶对建筑石膏凝结时间、强度、液相离子浓度与过饱和度,以及二水石膏晶体形貌和硬化体孔结构的影响,分析了石膏强度损失的内在原因.结果表明:骨胶对建筑石膏有显著的缓凝作用,它对建筑石膏强度的负面影响大大低于小分子类缓凝剂;骨胶对二水石膏晶体形貌和硬化体孔隙率影响较小,但使二水石膏晶体尺度增大,孔径分布粗化,这正是石膏强度降低的内在原因. Influence of one macromolecule-type retarder bone glue on the setting time, strength, ion concentration in liquid phase and supersaturation degree, crystal morphology of dehydrate and microstructure of hardened paste of building gypsum is investigated. Furthermore, internal cause of strength loss of building gypsum with addition of retarder is analyzed, The results indicate that bone glue could retard the hydration of building gypsum markedly, but its negative influence on the strength of building gypsum is far lower than that of low molecule-type retarders. Bone glue has a minor effect on crystal morphology of dehydrate and porosity of hardened paste, but it causes the large crystal size and coarsening of pore size distribution of hardened gypsum paste, which is the very intrinsic reason of strength loss of building gypsum.
出处 《重庆大学学报(自然科学版)》 EI CAS CSCD 北大核心 2006年第12期65-67,71,共4页 Journal of Chongqing University
基金 国家自然科学基金资助项目(50078055)
关键词 石膏 缓凝剂 晶体形貌 孔结构 gypsum retarder crystal morphology pore structure
  • 相关文献

参考文献8

二级参考文献9

共引文献62

同被引文献116

引证文献9

二级引证文献44

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部