摘要
研究自制交联剂FC-100在蚕蛹蛋白纤维活性染料染色中的应用.试验结果表明,在固色30 min后加入适量交联剂FC-100,能提高固色率,降低蚕蛹蛋白纤维的失重率,提高纤维的强力;交联剂用量以0.8 %~1.0 %为宜.
The application of self-synthesized cross-linker FC-100 to pupa protein fiber dyeing with reactive dyes is researched. The results show that the crosslinking agent added after 30 min fixation is helpful in exhaustion and maintenance of the fiber's weight and strength. The dosage of crosslinking agent is 0.8 % ~ 1.0 %.