摘要
对比研究干湿法混炼能耗和胶料性能。结果表明,与干法混炼相比,湿法混炼(高温雾化干燥)可减少粉尘污染,降低混炼功率约30%,提高填料的分散性能,大幅提升硫化胶的物理性能,降低滚动阻力,有助于混炼的节能环保,提高橡胶制品的性能。
The energy consumption and compound properties of dry and wet mixing process(high temperature atomization drying)were comparatively studied. The results showed that,compared with dry mixing,the wet mixing not only reduced dust pollution and decreased power consumption by about 30%,but also greatly improved the dispersion of fillers,substantially improved the comprehensive physical properties of the vulcanizates,and reduced rolling resistance. The wet mixing process was energy-saving and environmentally friendly, and improved the performance of rubber products.
作者
玄书鹏
边慧光
宋凤鹏
刘洁
汪传生
XUAN Shupeng;BIAN Huiguang;SONG Fengpeng;LIU Jie;WANG Chuansheng(Yiyang Rubber & Plastic Machinery Group Co.,Ltd,Yiyang 413000,China;Qingdao University of Science and Technology,Qingdao 266061,China)
出处
《橡胶工业》
CAS
2019年第2期134-137,共4页
China Rubber Industry
基金
山东省科技发展计划项目(2013TD16006)
山东省高等学校科技计划项目(J15LB73)
青岛市应用基础研究计划项目(16-5-1-100-jch)
山东省成果转化项目(2014CGZH0405)
关键词
湿法混炼
干法混炼
高温雾化
功率
分散性
滚动阻力
环保
wet mixing
dry mixing
high temperature atomization
power
dispersion
rolling resistance
environmentally friendly