期刊文献+

福建某锌精矿铜钼综合回收试验研究

Experimental study on copper-molybdenum comprehensive recovery from a zinc concentrate in Fujian
下载PDF
导出
摘要 福建某锌选矿厂的锌精矿含锌47.33%、含铜1.29%、含钼0.49%,铜、钼一直未得到有效回收。针对该锌精矿,开展再磨脱药—铜钼混合浮选—铜钼分离流程试验研究,铜钼混合浮选采用一粗两扫三精—粗精矿再磨工艺流程,铜钼分离采用一粗一扫四精工艺流程。全流程闭路试验可得到含铜20.11%、含金0.78 g/t、铜回收率65.9%的铜精矿,含钼39.49%、含铼18.28 g/t、钼回收率93.0%的钼精矿,以及含锌49.53%、锌回收率99.0%的锌精矿,有效降低了锌精矿中铜、钼杂质含量,同时得到了铜精矿和钼精矿产品,实现了锌、铜、钼的高效分离。 The zinc concentrate of a zinc beneficiation plant in Fujian contains 47.33%zinc,1.29%copper,and 0.49%molybdenum,with copper and molybdenum not effectively recovered.For this zinc concentrate,experimental research was conducted using a regrinding and agent removal-copper and molybdenum mixed flotation-copper and molybdenum separation process.The copper and molybdenum mixed flotation process employed a roughing stage,two scavenging stages,and three cleaning stages,followed by regrinding of the roughing concentrate,while the copper and molybdenum separation process included a roughing stage,a scavenging stage,and four cleaning stages.The closed-circuit test of the entire process yielded a copper concentrate containing 20.11%copper and 0.78 g/t gold,with a copper recovery rate of 65.9%;a molybdenum concentrate containing 39.49%molybdenum and 18.28 g/t rhenium,with a molybdenum recovery rate of 93.0%;and a zinc concentrate containing 49.53%zinc,with a recovery rate of 99.0%.This effectively reduced the impurities of copper and molybdenum in the zinc concentrate,while obtaining high-quality copper and molybdenum concentrates,achieving efficient separation of zinc,copper,and molybdenum.
作者 周生海 Zhou Shenghai(Zijin Mining Group Co.,Ltd.)
出处 《黄金》 CAS 2024年第6期31-36,共6页 Gold
基金 福建省科技计划项目(2017I1010) 厦门市留学人员科研项目(厦人社[2022]205号)。
关键词 锌精矿 再磨脱药 混合浮选 铜钼分离 综合回收 zinc concentrate regrinding and agent removal mixed flotation copper and molybdenum separation comprehensive recovery
  • 相关文献

参考文献10

二级参考文献133

共引文献65

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部