摘要 作为涂层前处理最重要的一道工序,超声清洗能将涂层产品表面油污、灰尘及氧化杂质清除,保证待镀产品表面清洁,提高膜基结合力。因此,本文研究超声波清洗机以及清洗液更换频次对PVD镀膜的AlCrSiN涂层铣刀的寿命的影响,通过两组对照实验,得出以下结论。第一,进口2CRD200全自动清洗设备比国产九槽清洗机清洗效果好,产品走刀寿命能提高24.09%。第二,使用2周以上的超声波清洗液清洗的刀具测试走刀寿命为2.91m,更换新超声波清洗液清洗的刀具测试走刀寿命为2.73m,频繁更换清洗液(两周一次)对提高产品待镀件清洁度,延长刀具走刀寿命影响不大。 As the most important process of coating pretreatment,ultrasonic cleaning can remove oil,dust and oxidized impurities on the surface of the coated product,ensuring the surface of the product to be coated is clean,and improving the adhesion of the film base.Therefore,this article studies the impact of ultrasonic cleaning machine and cleaning fluid replacement frequency on the life of PVD-coated AlCrSiN coated milling cutters.Through two sets of comparative experiments,the following conclusions are drawn.First,the imported 2CRD200 cleaning equipment has a better cleaning effect than the domestic nine-slot cleaning machine,and the tool life of the product can be increased by 24.09%.Second,the test tool life of tools cleaned with ultrasonic cleaning fluid for more than 2 weeks is 2.91m,and the test tool life of tools cleaned with new ultrasonic cleaning fluid is 2.73m.Frequent replacement of cleaning fluid(once every two weeks)improves the product.The cleanliness of the parts to be plated has little effect on extending the tool life.
作者 郭子铭 林荣川 GUO Zi-ming;LIN Rong-chuan(College of Marine Equipment and Mechanical Engineering,JiMei University,Xiamen 361021,China)
出处 《内燃机与配件》 2021年第20期68-69,共2页 Internal Combustion Engine & Parts
关键词 超声波清洗液 PVD镀膜 刀具寿命 ultrasonic cleaning fluid PVD coating tool life
  • 相关文献

参考文献5

二级参考文献32

  • 1Ed Lamm,梁治齐,李静.神奇的超声波清洗工艺[J].洗净技术,2003(2):65-68. 被引量:11
  • 2张继锋.超声波清洗在生产线中的应用[J].金属制品,2005,31(1):23-24. 被引量:7
  • 3陈辉,强颖怀,葛长路.超声波空化及其应用[J].新技术新工艺,2005(7):63-65. 被引量:46
  • 4李泉伟,杜春雨,俞宏星.超声波清洗技术在焊丝生产中的应用[J].金属制品,2006,32(1):13-14. 被引量:3
  • 5张而耕,吴雁.现代PVD表面工程技术及应用[M].北京:科学出版社,2013. 被引量:5
  • 6Kang M C, Tak H S, Jeong Y K, et al. Properties and tool performance of ta-C films deposited by double- bend filtered cathodic vacuum arc for micro drilling ap- plications[ J]. Diamond and Related Materials,2010, 19(7-9) :866-869. 被引量:1
  • 7Kao W H. High-speed drilling performance of coated micro-drills with Zr- C : H : Nx% coatings [ J ]. Wear, 2009,267 ( 5 - 8 ) : 1068 - 1074. 被引量:1
  • 8Kang M C, Je S K, Kim K H, et al. Cutting performance of CrN-based coatings tool deposited by hybrid coating method for micro drilling applications [ J ]. Surface and Coatings Technology,2008,202 ( 22-23 ) :5629-5632. 被引量:1
  • 9Chu C W, Jang J S, Chen H W, et al. Enhanced wear resistance of the Cr-based thin film coating on micro drill by doping with W-C- N [ J ]. Thin Solid Films, 2009,517(17) :5197-5201. 被引量:1
  • 10Wu Tao, Cheng Kai. An investigation on the micro cutting performance of diamond-like carbon coatings using finite element method [ J ]. The International Journal of Advanced Manufacturing Technology,2014, 73(9-12) :1321-1340. 被引量:1

共引文献104

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部