摘要
为了探讨含锌球团的较佳还原工艺,本文首先对内配碳含锌球团进行了脱水抗压试验,得出较佳的球团烘干条件:烘干温度200oC,时间120 min。并在1200℃下进行了球团还原试验得出球团较佳的直径及质量参数:球团直径12 mm,球团质量20 g。
In order to investigate the reduction behavior and optimum reduction process of zinc-containing pellets,the kinetic analysis of the reduction of zinc-containing pellets in the inner carbon is firstly carried out.It is concluded that the main limiting factors in the middle and late stages of the reaction are carbon gasification rate.The reaction rate at the interface of the zinc-containing pellets and the later diffusion.Then through the pellet compression test and pellet reduction experiment,the best pellet drying conditions and reduction conditions are obtained:drying temperature 200℃,time 120min,reduction temperature 1200℃,time 25min,pellet diameter 12 mm,pellet quality 20 g.
作者
蒋武锋
马腾飞
郝素菊
赵朔
张玉柱
Jiang Wufeng;Ma Tengfei;Hao Suju;Zhao Shuo;Zhang Yuzhu(College of Metallurgy and Energy,North China University of Science and Technology,Key Laboratory of Modern Metallurgy Technology,Ministry of Education,Tangshan,Hebei,China)
出处
《矿产综合利用》
CAS
北大核心
2020年第3期180-184,共5页
Multipurpose Utilization of Mineral Resources
基金
国家自然科学基金(NO.51274084)
河北省自然科学基金(E2018209323,E2017209231)
华北理工大学项目GP201507。
关键词
配碳
含锌球团
烘干
还原
Carbonation
Kinetics
Zinc-containing pellets
Reduction