摘要 通过分析影响高碳45号钢板坯角部横裂的钢水成分、结晶器锥度和冷却、设备对中精度、二冷水工艺等因素,提出了改善板坯角部横裂的有效措施,45号钢种板坯角横裂发生率由原来的8.61%降低到0.51%,角横裂得到有效控制。 Based on the analysis of the components of molten steel,the taper and cooling of mold,the accuracy of the equipment and the technological factors of secondary cooling water,the effective measures to improve the transverse corner cracks of No.45 steel are put forward,the rate of transverse corner cracks of No. 45 steel billet decreased from 8.61% to 0.51%,and the transverse corner cracks were effectively controlled.
作者 杨晓江 李中华 张大勇 周朝刚 YANG Xiao-jiang;LI Zhong-hua;ZHANG Da-yong;ZHOU Chao-gang(HBIS Laoting Iron and Steel Co., Ltd., Tangshan 063016, Hebei, China;College of Metallurgy and Energy, North China University of Science and Technology, Tangshan 063009, Hebei,China)
出处 《连铸》 2019年第2期35-38,共4页 Continuous Casting
关键词 板坯连铸 45号钢 角横裂 二冷水 结晶器 对弧精度 continuous casting slab No.45 steel transverse corner cracks second-cooling water mold taper equipment accuracy
  • 相关文献

参考文献5

二级参考文献23

共引文献122

同被引文献17

引证文献3

二级引证文献5

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部