本文在早期选矿实验的基础上,改进了选矿工艺流程,经过“一次粗选、四次扫选、一次精选”后,可获得金品位37.5×10-6,回收率87.17%的金精矿,达到了较为理想的工艺流程指标,回收率与原生产工艺相比,得到了较大的提高。
On the basis of early ore dressing experiment, this paper improves the process flow of mineral processing, after "one rough election, four sweep, one selection", can obtain gold grade 37.5×10-6, recovery rate of 87.17% gold concentrate, reached the ideal process flow index, Compared with the original production process, the recovery rate has been greatly improved.