摘要 基于雨雪天气后低阶煤焦自燃高发的现象,采用固定床管式炉在105~800℃范围内对褐煤提质,提质新鲜样(SA)及其水分复吸样(SC)分别在程序升温装置中进行自燃测定,分析自燃特性变化。结果显示,水分复吸使SC的临界温度吸氧量比SA降低60%以上。与SA不同,SC的吸氧量在低温氧化阶段很小且存在波动,在加速氧化阶段产生短暂"平台"期。SC在加速氧化阶段的瞬时升温速率(θ)比SA增加更快,自热温升加速。FCC指标显示,200~400℃提质的SC,自燃倾向性比SA显著增加,与SA-105接近,即高湿度环境储存会抵消提质降低褐煤自燃倾向性的效果。 In order to analyze the difference of spontaneous combustion characteristics between the fresh samples upgraded( SA) from 105℃ to 800℃ in fixed bed reactor and their samples suffering moisture re-adsorption( SC),the oxygen adsorbed and heating rate is obtained through oxidation test of temperature programming. The results show that the absorbed oxygen at critical temperature for SC reduced exceeding 60% comparing with SA. But catalytic action of water resulted in that the increase for instantaneous heating rate of SC is quicker than SA at the acceleraed oxidation stage,which means the self-heating for SC is faster. Based on assessment of FCC,the spontaneous combustion liability for SC upgraded at 200 ~400℃ went distinctly beyond SA. So storing at high moisture environment could counteract the effect that upgrading reduced the spontaneous combustion liability for lignite.
出处 《煤炭工程》 北大核心 2016年第10期131-134,共4页 Coal Engineering
基金 国家自然科学基金资助项目(U1261101) 国家重点基础研究发展规划资助项目(973计划 2014CB744301)
关键词 热提质 自燃特性 水分复吸 交叉点温度 吸氧量 升温速率 thermal upgrading spontaneous combustion characteristics moisture re-adsorption crossing point temperature absorbed oxygen heating rate
  • 相关文献

参考文献4

二级参考文献33

共引文献38

同被引文献11

引证文献2

二级引证文献14

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部