通过L9(34)正交试验 ,选择具有合适分子量的聚马来酸(PMA)无醛防皱整理剂和最优防皱整理工艺。并对棉织物进行防皱整理 ,获得良好的防皱整理效果 ,WRA值可达到243.5°,断裂强度保留率在70 %以上。
Through L9(34) orthogonal test, non-formaldehyde crease proofing agent polymaleic acid (PMA) with proper molecular weight and the optimal anti-crease finishing process were selected. The cotton fabric treated with this agent had got good wrinkle resistant result with WRA up to 243.5 and retained breaking strength more than 70%. Furthermore, synthetic process of PMA were optimized.