云南某低品位钨锡矿选矿试验研究 被引量:7

Study on dressing experiments of one low-grade tungsten and tin ore in Yunnan
下载PDF
导出
摘要 云南某钨锡矿含钨0.323%,锡0.140%,二氧化硅63.13%,三氧化二铝17.44%,氧化钙2.92%,氧化镁2.44%,在矿石工艺矿物学及试验研究的基础上,采用一段磨至-0.5mm,针对不同的床型,开展水力分级,进行摇床粗选,混合精矿脱硫、除铁、常温浮选分离钨锡的选矿工艺,获得了钨精矿产率0.31%,钨品位71.06%,钨回收率67.69%,含锡0.56%;锡精矿产率0.12%,锡品位58.18%,锡回收率50.94%,含钨3.80%,锡富中矿产率0.21%,锡品位4.22%,锡回收率6.87%,含钨2.69%,综合锡回收率57.81%的技术指标。 Experiments were carried out on one wolfram and tin ore which obtains tin (0 .140% ) ,silica (63 .13% ) ,aluminum oxide (17 .44% ) ,calcium oxide (2 .92% ) ,magnesium oxide (2 .44% ) in Yunnan . Based on the study on ore mineralogy and experimental study ,the ore was milled to -0 .5mm ,the process was as follows :firstly hydraulic separation was taken according to different type of beds ,then desulfidation and deironing were carried out ,after that separation of wolfram and tin was carried out by flotation at ordinary temperature .Productivities of concentrates of wolfram and tin are 0 .31% with wolfram (71.06% ) ,tin (0 .56% ) and 0 .12% with tin (58 .18% ) ,wolfram (3 .80% ) respectively .The recoveries of wolfram and tin are 67 .69% and 50 .94% in concentrates .Meanwhile productivity of middling of tin is 0 .21 with tin (4 .22% ) ,wolfram (2 .69% ) .The recovery of tin is 6 .87% in middling .Comprehensive recovery of tin is 57 .81% .
作者 李伟
出处 《中国矿业》 北大核心 2014年第6期135-139,共5页 China Mining Magazine
关键词 白钨矿 锡石 摇床粗选 钨锡分离 ore-forming fluid cassiterite rough selection of shaking table W-Sn separation
  • 相关文献

参考文献3

二级参考文献6

共引文献10

同被引文献169

引证文献7

二级引证文献15

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部