摘要 采用球磨制粉和模压成形方法制备铁硅铝磁粉芯,研究了退火温度、成型压力、磁粉粒度和磁粉热处理对磁粉芯的磁导率和损耗性能的影响。结果表明,提高退火温度和成型压力,磁粉芯的磁导率增大,损耗减小。磁粉粒度越小,磁粉芯的磁导率和磁芯损耗越低。磁粉在560℃热处理1小时后,磁粉芯的磁导率和损耗均降低。 FeSiAl.magnetic powder core was prepared from ball milled powders followed by molding. The permeability and power loss of magnetic powder core have been studied by changing annealing temperature, shaping pressure, granularity and magnetic powder heat treatment. The results indicated that increasing annealing temperature and shaping pressure can increase permeability and decrease power loss of magnetic powder core. Decreasing granularity of magnetic powder can reduce the permeability and power loss of magnetic powder core. Heat treatment can decrease the permeability and power loss of magnetic powder core.
作者 金丹 孙可为
出处 《材料科学与工程学报》 CAS CSCD 北大核心 2012年第4期525-527,共3页 Journal of Materials Science and Engineering
基金 陕西省教育厅科研计划资助项目(09JK526) 西安建筑科技大学科技基金资助项目(JC0916)
关键词 铁硅铝磁粉芯 磁导率 损耗 退火处理 FeSiA1 magnetic powder core permeability core losses annealing treatment
  • 相关文献

参考文献9

二级参考文献21

共引文献71

同被引文献83

引证文献8

二级引证文献23

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部