摘要
完成了铁水热装入 50 t超高功率电弧炉的试验,节能效果显著,电耗降低 30-10 kW·h/t,平均为 50 kW·h/t;冶炼时间缩短 5—20 min平均 7 min.并对影响冶炼电耗、时间的关键问题进行了分析.
The test of adding liquid iron into 50 t ultrahight power electric arc furnace (EAF) has been successfully finished, and the results show that the projection, the consume power decreases 30-100 kW·h/t (averge 50 kW.h/t) and the smelting time 5-20 min (average 7 min). In this paper, the factors affecting the consume electricity and the smelting time are analysed.