按照GB/T 8814—2004《门、窗用未增塑聚氯乙烯(PVC-U)型材》进行了4 000h老化试验,考察了样品ΔE*、Δb*和光泽度的变化。结果表明:①所有样品在2 000h时都出现了变色峰值,而且峰值都超过GB/T8814—2004的规定,但到4 000h时样品的变色情况反而达标;②PVC型材表面颜色的变化不仅是PVC老化的结果,同时也是其表面粉化的结果;③GB/T 8814—2004对PVC型材耐候性的检测方法存在不足,应适当地对样品的老化过程进行跟踪和评估。
Ageing test of 4 000 h are carried out according to GB/T 8814- 2004 Unplasticized Pol yvinyl Chloride ( PVC-U) Profiles for the Fabrication of Doors and Windows to investigate samples' changes in △E* , △b* and glossiness. The results show that (1) discoloration of all the samples appears peak value at 2 000 h and all the peak value exceed the specified value in GB/T 8814 - 2004, but the discoloration of all the samples at 4 000 h reaches to the standard; (2) not only PVC's ageing but also its surface chalking contributes to change in surface color of PVC profiles; (3) there are shortcomings in the test method of weather resistance of PVC profiles in GB/T 8814 - 2004, and thus the samples' ageing process should be tracked and evaluated appropriately.
出处
《聚氯乙烯》
CAS
2012年第3期28-30,共3页
Polyvinyl Chloride
关键词
PVC型材
耐候性
粉化
标准
检测
PVC profile
weather resistance
chalking
standard
test