摘要 以UO22+为印迹离子,偶氮二异丁腈(AIBN)为引发剂,邻苯二酚-UO22+-4-乙烯基吡啶三元配合物为模板,与苯乙烯单体、交联剂二乙烯基苯在甲醇溶液中通过共聚反应制备了UO22+印迹聚合物微球。该印迹聚合物微球经6mol/L HCl处理后留下与铀酰离子大小相匹配的空穴,对水溶液中微量铀有富集作用,在pH=5~7及吸附时间在20min以上时,该印迹聚合物微球对水溶液中微量铀的吸附率可达99%以上,且具有良好的选择性;HCl浓度在1.0mol/L以上,淋洗体积为聚合物体积的5倍以上,淋洗时间在20min以上时洗脱率可达99%以上。将其应用于卤水中微量铀的测定,与标准方法相比较,所得结果令人满意。 Uranyl ion imprinted polymer beads were prepared by the copolymerization of styrene monomer and divinyl benzene as crosslinking agent in methanol solution,with the UO2+2-o-dihydroxybenzene-4-vinyl pyridine ternary complex as template,the 2,2′-azo-bis-isobutyronitrile as initiator and UO2+2 as the imprinting ion.The uranyl ions were removed from the polymer beads by treating with 6 mol/L HCl,leaving behind cavities that match uranyl ion in size.The treated polymer beads can preconcentrate uranyl ions from dilute aqueous solutions.The adsorption efficiency can reach 99% or above with good selectivity when pH is in the range of 5-7 and the adsorption time is more than 20 min.The elution rate can reach above 99% under the conditions of concentration of HCl being above 1.0 mol/L,elution time more than 20 min and the elution volume more than 5 times the volume of ion imprinted polymer.The uranyl ion imprinted polymer beads have been successfully applied to determine micro-uranium in brine samples.The results are satisfactory compared with NBS method.
出处 《原子能科学技术》 EI CAS CSCD 北大核心 2011年第3期267-271,共5页 Atomic Energy Science and Technology
基金 国家自然科学基金资助项目(20707008) 湖南省自然科学基金资助项目(07JJ5004)
关键词 铀酰离子 三元配合物 印迹聚合物 卤水 uranyl ion ternary complex ion imprinting polymer brine
  • 相关文献

参考文献13

  • 1小宫山真,等.分子印迹学-从基础到应用[M].吴史康,汪鹏飞,译.北京:科学出版社,2006:8-11. 被引量:14
  • 2罗明标,李伯平,杨枝,刘维,龚治湘.铀(Ⅵ)分析中的分离富集技术[J].铀矿地质,2008,24(1):57-62. 被引量:7
  • 3任俊树,牟涛,张惟,杨胜亚.废水组分对离子交换树脂处理含铀废水的影响[J].原子能科学技术,2008,42(1):38-42. 被引量:6
  • 4杜阳,邱咏梅,但贵萍,张东,雷家荣.海藻吸附水中铀离子初步研究[J].原子能科学技术,2007,41(4):416-419. 被引量:10
  • 5赵宝生,蔡青.离子浮选法处理放射性废水[J].原子能科学技术,2004,38(4):382-384. 被引量:10
  • 6GLADIS J M, RAO T P. Quinoline-8-ol-immobilized amberlite XAD-4: Synthesis, characterization, and uranyl ion uptake properties suitable for analytical applieations[J]. Analytical and Bioanalytical Chemistry, 2002, 373(8): 867-872. 被引量:1
  • 7GLADIS J M, RAO T P. eal applications of uranyl Synthesis and analytiion imprinted polymer particles[J]. Analytical Letters, 2003, 36 (10) 2 107-2 121. 被引量:1
  • 8METILDA P, GLADIS J M, VENKATESWARAN G, et al. Investigation of the role of chelating ligand in the synthesis of ion-imprinted polymeric resins on the selective enrichment of uranium(Ⅵ)[J]. Analytica Chimiea Acta, 2007, 587 (2) : 263-271. 被引量:1
  • 9PREETHA C R, GLADIS J M, RAO T P. Removal of toxic uranium from synthetic nuclear power reactor effluents using uranyl ion imprinted polymer particles[J]. Environ Sei Technol, 2006, 40(9): 3 070-3 074. 被引量:1
  • 10ROACH J D, ZAPIEN J H. Inorganic ligand-modi lied, colloid-enhanced ultrafiltration: A novel meth od for removing uranium from aqueous solution[J]. Water Res, 2009, 43(18) : 4 751-4 759. 被引量:1

二级参考文献43

共引文献49

同被引文献74

引证文献6

二级引证文献53

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部