Effect of Metallic Zn Powder on Oxidation Resistance of Al_2O_3-C Refractories 被引量:2

Effect of Metallic Zn Powder on Oxidation Resistance of Al_2O_3-C Refractories
下载PDF
导出
摘要 Al2O3-C specimens were prepared by using tabular corundum, flaky graphite, Al, Si, and Zn powder as starting materials and phenolic formaldehyde resin as binder. Keeping the mass ratios of tabular corundum, flaky graphite, Al and Si constant, different contents of Zn (0,0. 5%, 1%, 2% and 3% ) were added respectively. The specimens were/teat treated at 120 -220℃ for 24h, and then fired at 1400℃ for 3h in air atmosphere. The mass change rate, thickness of decarburization layer, apparent porosity, bulk density and microstructure of the products were determined and observed by means of SEM and EDX. The results show that the specimen with 2% Zn was characterized by minimum in thickness of decarburization layer and in apparent porosity and maximum in bulk density. Consequently, the specimen with 2% metal Zn is supposed to perform the best oxidation resistance. Al2O3-C specimens were prepared by using tabular corundum, flaky graphite, Al, Si, and Zn powder as starting materials and phenolic formaldehyde resin as binder. Keeping the mass ratios of tabular corundum, flaky graphite, Al and Si constant, different contents of Zn (0,0. 5%, 1%, 2% and 3% ) were added respectively. The specimens were/teat treated at 120 -220℃ for 24h, and then fired at 1400℃ for 3h in air atmosphere. The mass change rate, thickness of decarburization layer, apparent porosity, bulk density and microstructure of the products were determined and observed by means of SEM and EDX. The results show that the specimen with 2% Zn was characterized by minimum in thickness of decarburization layer and in apparent porosity and maximum in bulk density. Consequently, the specimen with 2% metal Zn is supposed to perform the best oxidation resistance.
出处 《China's Refractories》 CAS 2006年第4期29-33,共5页 中国耐火材料(英文版)
关键词 Corrosion mechanism MgO-CaO Refractory ANTIOXIDANT Oxidation resistance Corrosion mechanism, MgO-CaO Refractory, Antioxidant, Oxidation resistance
  • 相关文献

参考文献1

二级参考文献28

  • 1Knochel, P. J. Am. Soc. Chem. 1991, 113, 5735. 被引量:1
  • 2Adrian, J. C.; Barkin, J. L.; Hassib, L. Tetrahedron Lea. 1999, 40, 2457. 被引量:1
  • 3Rieke, R. D. Science 1987, 246, 1260. 被引量:1
  • 4Chou, W. N.; Clark, D. L.; White, J. B. Tetrahedron Lett. 1991, 32, 299. 被引量:1
  • 5Solladie, G.; Stone, G. B.; Andres, J. M.; Urbano, A. Tetrahedron Lett. 1993, 34, 2835. 被引量:1
  • 6Petrier, C.; Luche, J. L. Tetrahedron Le tt. 1987, 28, 2347. 被引量:1
  • 7Comins, D. L.; Brooks, C. A.; Ingalls, C. L. J. Org. Chem. 2001, 66, 2181. 被引量:1
  • 8(a) Wang, W. B.; Shi, L. L.; Huang, Y. Z. Tetrahedron Lett. 1990, 31, 1185.(b) Kardile, G. B.; Desai, D. G.; Swami, S. S. Synth. Commun. 1999, 29, 2129.(c) Mukhopadhyay, S.; Rothenerg, G.; Wiener, H.; Sasson, Y. New J. Chem. 2000, 24, 305.(d) Rosnati, V. Tetrahedron Lett. 1992, 33, 4791.(e) Li, G. P.; Jiang, H. F.; Li, J. H. The11thIUPAC International Symposium on Organo-metallic Chemsitry Directed towards Organic Synthesis, Taipei, 2001, p. 52. 被引量:1
  • 9(a) Li, T.;Cui, W.;Liu, J.G.;Zhao, J.Z.;Wang, Z. G. Chem. Commun. 2000, 139.(b) Rani, B. R.; Ubukata, M.; Osada, H. Bull. Chem. Soc. Jpn. 1995, 68, 282. (c) Delair, P.; Luche, J. L. J. Chem. Soc., Chem.Commun. 1989, 398. 被引量:1
  • 10Vona, M. L. D.; Floris, B.; Luchetti, L.; Rosnati, V. Tetrahedron Left. 1990, 42, 6081. 被引量:1

共引文献5

同被引文献31

引证文献2

二级引证文献4

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部