摘要
利用溶剂在层状液晶中的渗透性,和层状液晶中溶剂厚度的限定性,在TritonX-100/C10H21OH/H2O体系层状液晶中,以24.0%(质量分数)KCl水溶液代替组分水,制备水溶性超微粒子材料KCl,粒径大小约为4~6nm.
Water-soluble fine KCl particle was prepaxed by replacing component water with 24.0% KCl aqueous solution in the Triton X-100/C10H21OH/H2O lamellar liquid crystal. The preparation was based on the penetration of solvent in the lamellar liquld crystat and the limitation of the change of thickness of solvation layer in the lamellar liquid crystal. The size of water-soluble fine particle KCl was about 4-6nm.