合成了一系列易水解聚酯(EHDPET),研究了第三、四单体含量及添加剂B对EHDPET流变性能的影响,得到了EHDPET的粘流活化能与剪切速率之间的关系。结果表明,EHDPET的流动性能随第三单体(SIPE)含量的增加而下降,增大第四单体(脂肪族化合物A)的添加量和添加聚合物B均可使EHD-PET的流动性能得到改善。
Easy hydrolysis degradable polyester (EHDPET) is an ideal material for manufacturing super-fine fiber by blend spinning or composite spinning. A series of EHDPET had been synthesized by PTA process and a rheology study was carried out to investigate the influence of the content of the third monomer (SIPE), forth monomer (aliphatic A) and additive B. The relation between visco-flow activition energy and shear rates was also described. The result shows that the rheological properties become worse as the content of SIPE increases; adding more aliphatic polymer A and adding B can both improve the flow behavior of EHDPET.
出处
《高分子材料科学与工程》
EI
CAS
CSCD
北大核心
2004年第5期200-202,207,共4页
Polymer Materials Science & Engineering
基金
国家自然科学基金资助项目(59973002)