PHASE TRANSFORMATION AND CHARACTERISTICS IN FRECKLE AREAS FOR INCONEL 625 SUPERALLOY 被引量:11
1
作者 J.X.Dong M.C.Zhang Y.P.Zeng X.S.Xie 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2005年第1期47-54,共8页
The freckle formation and their phase characterizatics in freckle areas were investigated by means of microstructure analysis approaches and a thermodynamic equilibrium phase calculation method in an Inconel 625 allay... The freckle formation and their phase characterizatics in freckle areas were investigated by means of microstructure analysis approaches and a thermodynamic equilibrium phase calculation method in an Inconel 625 allay. These results show that in freckle areas a large number of M6C, MC, Laves and δ phases precipitate in grain boundaries even within grain due to the enrichment and segregation of Mo and Nb during solidification, which results in almost of these freckle areas covered by these complex precipitated phases and induces small grains in freckle areas. Equilibrium phase and liquid segregation calculation can give a reasonable interpretation of the freckle feature for this alloy. 展开更多
关键词 FRECKLE superalloy Inconel 625 thermodynamic calculation
下载PDF
均匀化处理对铸态GH625合金组织的影响 被引量:5
2
作者 李红梅 聂义宏 +1 位作者 张鑫 白亚冠 《材料热处理学报》 EI CAS CSCD 北大核心 2019年第3期75-81,共7页
利用光学显微镜、扫描电镜和能谱分析等研究了采用真空感应熔炼和保护气氛电渣重熔工艺生产的GH625合金的铸态组织和均匀化热处理后的微观组织。结果表明:采用双联工艺生产的GH625合金电渣锭存在枝晶和元素偏析,其中Nb、Mo、Ti元素为主... 利用光学显微镜、扫描电镜和能谱分析等研究了采用真空感应熔炼和保护气氛电渣重熔工艺生产的GH625合金的铸态组织和均匀化热处理后的微观组织。结果表明:采用双联工艺生产的GH625合金电渣锭存在枝晶和元素偏析,其中Nb、Mo、Ti元素为主要偏析元素;均匀化热处理后枝晶消除明显,块状及条状碳化物碎化,棱角钝化;相同均匀化热处理工艺下Ti、Mo、Nb达到均匀化的难度依次加大;GH625合金最佳的均匀化热处理的工艺为1200℃保温24 h。 展开更多
关键词 625高温合金 显微结构 偏析 均匀化
原文传递
625合金凝固偏析的理论分析 被引量:5
3
作者 孙锋 梅林波 +1 位作者 刘松锋 于文龙 《热力透平》 2016年第1期46-50,共5页
利用材料性能模拟软件JMatPro 7.0与相应的Ni基高温合金数据库,对INCONEL 625合金的凝固偏析行为进行了分析,以帮助制定均匀化退火工艺及合金成分筛选。结果表明:625合金存在严重的Cr、Fe、Mo、Nb偏析。其中Nb是控制材料均匀化行为的最... 利用材料性能模拟软件JMatPro 7.0与相应的Ni基高温合金数据库,对INCONEL 625合金的凝固偏析行为进行了分析,以帮助制定均匀化退火工艺及合金成分筛选。结果表明:625合金存在严重的Cr、Fe、Mo、Nb偏析。其中Nb是控制材料均匀化行为的最主要元素,Mo次之。通过加Ti、减Si可抑制Mo的偏析;加C减少Fe、Cr则可有效抑制Nb偏析。为使退火时间控制在合理范围内,有必要采取1 200℃高温退火。 展开更多
关键词 高温合金 625合金 偏析 均匀化 汽轮机
下载PDF
基于挤压实验的高温合金IN625本构关系模型 被引量:3
4
作者 王忠堂 张士宏 +1 位作者 程明 李德富 《热加工工艺》 CSCD 北大核心 2014年第3期81-83,共3页
提出了一种基于挤压实验的材料本构关系模型的新方法,即根据管材挤压实验数据建立适合于管材挤压变形时的材料本构关系模型。在16.3MN挤压机上对高温合金IN625进行了热挤压试验研究。根据热挤压实验数据以及Arrhenius型材料本构模型,... 提出了一种基于挤压实验的材料本构关系模型的新方法,即根据管材挤压实验数据建立适合于管材挤压变形时的材料本构关系模型。在16.3MN挤压机上对高温合金IN625进行了热挤压试验研究。根据热挤压实验数据以及Arrhenius型材料本构模型,确定了高温合金IN625管材挤压变形的材料本构关系模型,该模型的计算结果和实验结果的相对误差小于7.8%。确定的本构关系模型的适用温度为1150~1200℃,应变速率为1.86~7.44 s^-1。 展开更多
关键词 高温合金 IN625 本构关系 挤压实验
下载PDF
GH625合金的热变形行为 被引量:11
5
作者 刘志超 周海涛 +1 位作者 李庆波 温盛发 《热加工工艺》 CSCD 北大核心 2010年第12期31-35,共5页
采用Gleeble-1500热模拟试验机研究了GH625高温合金在应变速率为0.001~1 s-1、变形温度为1223~1373 K条件下的热变形行为。结果表明:当变形温度一定时,随应变速率的升高,合金的峰值应力σp和稳态流动应力σs及对应的应变εp和εs均升... 采用Gleeble-1500热模拟试验机研究了GH625高温合金在应变速率为0.001~1 s-1、变形温度为1223~1373 K条件下的热变形行为。结果表明:当变形温度一定时,随应变速率的升高,合金的峰值应力σp和稳态流动应力σs及对应的应变εp和εs均升高;当变形速率一定时,随变形温度的升高,σp和σs以及εs均降低,但εp基本保持不变。GH625合金在热压缩变形过程中应变速率的降低和变形温度的升高均有利于动态再结晶的发生;根据应力-应变曲线,通过线性回归获得GH625合金的本构方程。 展开更多
关键词 GH625高温合金 热压缩变形 动态再结晶 真应力-真应变曲线 热变形的本构方程
下载PDF
Nucleation mechanisms of dynamic recrystallization in Inconel 625 superalloy deformed with different strain rates 被引量:8
6
作者 Guo, Qingmiao Li, Defu +3 位作者 Peng, Haijian Guo, Shengli Hu, Jie Du, Peng 《Rare Metals》 SCIE EI CAS CSCD 2012年第3期215-220,共6页
The effects of strain rates on the hot working characteristics and nucleation mechanisms of dynamic recrystallization (DRX) were studied by optical microscopy and electron backscatter diffraction (EBSD) technique. Hot... The effects of strain rates on the hot working characteristics and nucleation mechanisms of dynamic recrystallization (DRX) were studied by optical microscopy and electron backscatter diffraction (EBSD) technique. Hot compression tests were conducted using a Gleeble-1500 simulator at a true strain of 0.7 in the temperature range of 1000 to 1150 °C and strain rate range of 0.01 to 10.00 s?1. It is found that the size and volume fraction of the DRX grains in hot-deformed Inconel 625 superalloy firstly decrease and then increase with increasing strain rate. Meanwhile, the nucleation mechanism of DRX is closely related to the deformation strain rate due to the deformation thermal effect. The discontinuous DRX (DDRX) with bulging of original grain boundaries is the primary nucleation mechanism of DRX, while the continuous DRX (CDRX) with progressive subgrain rotation acts as a secondary nucleation mechanism. The twinning formation can activate the nucleation of DRX. The effects of bulging of original grain boundaries and twinning formation are firstly gradually weakened and then strengthened with the increasing strain rate due to the deformation thermal effect. On the contrary, the effect of subgrain rotation is firstly gradually strengthened and then weakened with the increasing strain rate. 展开更多
关键词 nucleation mechanisms dynamic recrystallization Inconel 625 superalloy deformation strain rate
下载PDF
高Cr高温合金中α-Cr相的析出方式 被引量:8
7
作者 董建新 张麦仓 +1 位作者 曾燕屏 谢锡善 《北京科技大学学报》 EI CAS CSCD 北大核心 2002年第2期186-190,共5页
通过对高Cr高温合金INCONEL718和INCONEL625在长期时效过程中α-Cr相析出方式进行详细的微观组织分析、结果认为,随着时效时间的延长,INCONEL718合金中大部分α-Cr相随着δ相的析出长大依附于... 通过对高Cr高温合金INCONEL718和INCONEL625在长期时效过程中α-Cr相析出方式进行详细的微观组织分析、结果认为,随着时效时间的延长,INCONEL718合金中大部分α-Cr相随着δ相的析出长大依附于δ相的界面析出,而INCONEL625合金中α-Cr相则主要依附晶界M6C碳化物相界面析出,少部分依附于δ相析出,其原因可能与Cr在δ相和M6C碳化物 中的溶解度随温度的下降而迅速下降有关. 展开更多
关键词 高Cr高温合金 Α-CR相 析出方式 高铬高温合金
下载PDF
高温合金差示扫描量热分析(DSC)的影响因素研究:合金状态和升/降温速率 被引量:6
8
作者 郑亮 刘玉峰 +7 位作者 刘杨 王悦 张轶波 刘娜 许文勇 袁华 李周 张国庆 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2019年第6期1944-1953,共10页
对固溶强化型镍基高温合金(625合金)进行升、降温差示扫描量热分析(DSC)试验,研究了同一合金不同状态(粉末态、热等静压态和铸态)以及升/降温速率(5~10℃/min)对相变温度的影响。采用场发射扫描电镜(FESEM)、电子探针(EPMA)对不同状态62... 对固溶强化型镍基高温合金(625合金)进行升、降温差示扫描量热分析(DSC)试验,研究了同一合金不同状态(粉末态、热等静压态和铸态)以及升/降温速率(5~10℃/min)对相变温度的影响。采用场发射扫描电镜(FESEM)、电子探针(EPMA)对不同状态625合金的微观组织和元素分布进行表征。结果表明:(1)铸态比粉末态合金的枝晶间距大2个数量级,而热等静压态合金为无枝晶偏析的细等轴晶结构。(2)升/降温速率对DSC曲线中加热时开始熔化温度(等于固溶强化型合金的初熔温度)和冷却时开始凝固温度(偏离基线的拐点)无影响,但对合金加热时熔化结束、冷却时大量凝固析出温度(峰位)和终凝温度(拐点)有明显影响。采用加热、冷却曲线相应相变温度平均值的方法可减少DSC试验和样品条件的影响,获得相对固定且更具可比性的合金相变温度。(3)合金状态对初熔温度和DSC加热曲线固相线附近的圆弧段有明显影响。根据DSC加热曲线固相线附近的圆弧大小可以判断合金的偏析倾向,弱偏析倾向的粉末态和热等静压态625合金DSC加热曲线固相线附近拐点尖锐,表现为合金开始熔化温度(偏离基线的拐点)与名义固相线温度(切线交点)差异很小,分别仅为5和6℃;偏析倾向较大的铸态625合金的DSC加热曲线中固相线附近为较大圆弧,开始熔化温度与名义固相线温度差异可达52℃。铸态625合金的初熔温度比热等静压态和粉末态分别低45和40℃,在实际热处理和热等静压等热工艺参数选择时应注意圆弧段较大的合金降低初熔温度的影响。在所有DSC冷却曲线中,由于完全熔化重新凝固消除了合金原始显微组织特征,不同状态625合金固相线附近曲线形态相似,均为较大的圆弧。 展开更多
关键词 镍基高温合金 625合金 DSC 粉末 热等静压 铸态组织 偏析
原文传递
Flow Behavior and Microstructures of Inconel 625 Superalloy at the Elevated Temperature 被引量:2
9
作者 Li Defu, Guo Shengli, Wu Zhigang, Zou Honghui, Pen Haijian General Research Institute for Nonferrous Metals, Beijing 100088, China 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2011年第S3期95-98,共4页
The deformation behavior of Inconel 625 superalloy was investigated by means of hot compression tests. The flow stress curves were obtained in the temperature and strain rate ranges of 950-1200 ℃ and 0.01-10 s-1, res... The deformation behavior of Inconel 625 superalloy was investigated by means of hot compression tests. The flow stress curves were obtained in the temperature and strain rate ranges of 950-1200 ℃ and 0.01-10 s-1, respectively. Optical microscopy was used to evaluate the microstructural evolution of the alloy under different conditions examined. The results show that the flow stress decreases with decreasing strain rate and increasing temperature, and the activation energy is about 654.502 kJ/mol. Microstructure observations show that with increasing temperature, the sizes and volume fraction of dynamic recrystallization (DRX) grains increase. The strain has no remarkably effect on the sizes of DRX grains, but with increasing strain the volume fraction of DRX grains increases. During hot compression of Inconel 625 superalloy at elevated temperature, the occurrence of DRX was the main softening mechanism. The DRX mechanism of Inconel 625 superalloy can be mainly attributed to the discontinuous dynamic recrystallization (DDRX). 展开更多
关键词 INCONEL 625 superalloy HOT DEFORMATION flow stress dynamic RECRYSTALLIZATION
原文传递
高温合金差示扫描量热分析(DSC)的影响因素:粉末粒度和显微组织 被引量:3
10
作者 郑亮 刘玉峰 +5 位作者 Gorley Michael J Hong Zuliang DaySarah Tang Chiu C 李周 张国庆 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2019年第5期1591-1597,共7页
对固溶强化型625镍基高温合金粉末进行升、降温差示扫描量热分析(DSC)试验,研究了不同粉末粒度(<37,45~53,75~105,105~150,150~355μm)对相变温度的影响。采用场发射扫描电镜(FESEM)、电子探针(EPMA)和同步辐射X射线衍射(SXRD)对625... 对固溶强化型625镍基高温合金粉末进行升、降温差示扫描量热分析(DSC)试验,研究了不同粉末粒度(<37,45~53,75~105,105~150,150~355μm)对相变温度的影响。采用场发射扫描电镜(FESEM)、电子探针(EPMA)和同步辐射X射线衍射(SXRD)对625合金粉末的形貌、元素分布和相组成进行表征。结果表明:不同粒径PM625粉末均为树枝晶结构,枝晶间距在2~10μm范围,元素Ni和Cr倾向分布于枝晶干,Mo和Nb偏析于枝晶间。不同粒度的PM625粉末中均仅存在基体γ相。PM625粉末DSC加热曲线固相线附近区域拐点尖锐,表现为合金开始熔化温度(偏离基线的拐点)与名义固相线温度(切线交点)差异很小,不同粒度间的差异仅为2~5℃。合金完全熔化后重新冷却的过程中原始粉末的低偏析特性消失,冷却曲线固相线区域圆弧较大,名义固相线和终凝温度差较大,为53~65℃。DSC试验升温过程中不同粒径粉末的固、液相线以及初熔温度最大差异分别为3, 2和2℃,降温过程不同粒径粉末固、液相线温度差分别为6和2℃。0~355μm粉末粒径范围内,粒径对固溶强化型PM625高温合金粉末相变温度无明显影响。 展开更多
关键词 625镍基高温合金 差示扫描量热分析(DSC) 同步辐射XRD 粉末粒度 相变