摘要
介绍了用CO_2堆焊35CrMo钢钻井泵阀箱密封面磨损修复工作,通过试验表明,采用Φ1.2mm的H08Mn2Si焊丝,以短路过渡CO_2焊法施焊,可以获得致密、耐磨的堆焊金属层。该法已成功地用于生产,取得了良好的经济效益。
The paper introduces a method to repair the 35CrMo seal surface of valve box of drill pump by bead-on-plate CO, welding. The results show that it can get a high density and wear proof metal layer through using 1.2mm diameter wire H08Mn2Si and short-circuit metal transfer CO_2 welding. This method has been successfully applied in production and good economic profits have been attained.
出处
《材料科学与工艺》
EI
CAS
CSCD
北大核心
1993年第2期86-92,共7页
Materials Science and Technology
关键词
堆焊
泵阀箱
密封面
二氧化碳
钻井
bead-on-plate CO_x wclding
35CrMo steel
seal surface of pump valve box