金沉积烤瓷冠的临床应用与评价 被引量:3

Evaluation and clinical application of auro-galvano-crown(AGC)
下载PDF
导出
摘要 目的 评价金沉积烤瓷技术与其它烤瓷技术的临床修复效果。方法 对临床上进行金沉积烤瓷冠修复的51例共328件修复体进行随访。结果 在随访的312件修复体中309件成功,3件失败。其中1件为崩瓷,2件为粘结和固位问题。结论 金沉积烤瓷冠的修复效果要优于镍铬合金及铸造金合金烤瓷冠。金沉积烤瓷技术的优点在于:①生物相容性好。②冠边缘密合性好。③色泽自然美观。 Objective The aim of this study is to evaluate the clinical effectiveness of galvano-ceramic single crowns (Auro-galvano-crown, AGC) and the other porcelain fused metal (PFM) crowns. Methods A total 328 of galvano-ceramic single crowns (AGC) in 51 patients were reviewed for 3 years, respectively, after cementation. Results 309 crowns had successful results and 3 crowns were failures. 1 was for the fracture of ceramic and the other 2 were for the problem of cementation or restoration. Conclusion Long-term results of galvano-ceramic individual crown restorations were superior to those of the other porcelain fused metal (PFM) crown restorations (Including Ni-Cr and 86.2% Au Cast metal). The AGC (Auro-galvano-crown) technique has some advantages in that it provides the best biocompatibility, exquisite marginal integrity and natural color beneath the ceramics.
作者 陈丽萍 李玲
出处 《口腔材料器械杂志》 2004年第1期20-21,25,共3页 Chinese Journal of Dental Materials and Devices
关键词 金沉积烤瓷冠 临床应用 生物相容性 修复体 口腔修复材料 Auro-galvano-crown(AGC) Porcelain-fused-to-metal crown(PFM) All ceramic crown
  • 相关文献

参考文献2

二级参考文献10

  • 1Hae m merle CH,Mesaric W,Lang NP.Marginal fit of porcelain crowns with galvanized fra mes[].Schweizer Monatsschrift fur Zahnmedizin.1994 被引量:1
  • 2Holmes JR,Pilcher ES,Rivers JA,et al.Marginal fit of electroformed ceramometal crowns[].Journal of Prosthodontics.1996 被引量:1
  • 3Faber FJ.Verformung von galvanokera mschen kronen nach kera mischer verblendung[].Deutsche Zahnarztliche Zeitschrift.1997 被引量:1
  • 4Setz J,Diehl J,Weber H.Der Randschluss zementierter galvanokeramischer kronen[].Quintessenz.1989 被引量:1
  • 5Wirz J,Jaeger K,Schmidli F,et al.Moderne galvano technologie[].Schweizer Monatsschrift fur Zahnmedizin.1996 被引量:1
  • 6Gilde H.Untersuchungen zur druckbelastbarkeit von galvanokronen[].Zahnarztliche Welt.1991 被引量:1
  • 7Horn V,Kappert HF.Festigkeit von dreigliedrigen Galvanobruecken im Seitenzahnbereich[].Deutsche Zahnarztliche Zeitschrift.1992 被引量:1
  • 8Kaan B,Eichner K,Kaan M,et al.Untersuchungen des randschlusses von Galvano-Keramik-Inlays[].ZWR.1998 被引量:1
  • 9Schwickerath H.Die Keramisch verblendete galvanokrome[].Quintessenz Zahntechnik.1988 被引量:1
  • 10Erpenstein H,Kerschbaum TH.Frakturanfaelligkeit von glas-und galvanokeramischen kronen[].Deutsche Zahnarztliche Zeitschrift.1995 被引量:1

共引文献50

同被引文献18

引证文献3

二级引证文献9

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部