期刊文献+

Fluid-Related Performances and Compressive Strength of Clinker-Free Cementitious Backfill Material Based on Phosphate Tailings

下载PDF
导出
摘要 Phosphate tailings are usually used as backfill material in order to recycle tailings resources.This study considers the effect of the mix proportions of clinker-free binders on the fluidity,compressive strength and other key performances of cementitious backfill materials based on phosphate tailings.In particular,three solid wastes,phosphogypsum(PG),semi-aqueous phosphogypsum(HPG)and calcium carbide slag(CS),were selected to activate wet ground granulated blast furnace slag(WGGBS)and three different phosphate tailings backfill materials were prepared.Fluidity,rheology,settling ratio,compressive strength,water resistance and ion leaching behavior of backfill materials were determined.According to the results,when either PG or HPG is used as the sole activator,the fluidity properties of the materials are enhanced.Phosphate tailings backfill material activated with PG present the largest fluidity and the lowest yield stress.Furthermore,the backfill material’s compressive strength is considerably increased to 2.9 MPa at 28 days after WGGBS activation using a mix of HPG and CS,all with a settling ratio of only 1.15 percent.Additionally,all the three ratios of binder have obvious solidification effects on heavy metal ions Cu and Zn,and P in phosphate tailings.
出处 《Fluid Dynamics & Materials Processing》 EI 2024年第9期2077-2090,共14页 流体力学与材料加工(英文)
基金 the Key Research and Development Program of Hubei Province(2022BCA071) the Wuhan Science and Technology Bureau(2022020801020269).
  • 相关文献

参考文献1

二级参考文献6

  • 1WAN Huiwen, SHUI Zhonghe, LIN Zongshu. Analysis of geometric characteristics of GBFS particles and their influences on cement properties [J]. Cem Concr Res, 2004, 34(1): 133-137. 被引量:1
  • 2EDINGER S E. The growth of gypsum [J]. J Cryst Growth, 1973(18): 217-223. 被引量:1
  • 3MUN K J, HYOUNG W K, LEE C W. Basic properties of non-sintering cement using phosphogypsum and waste lime as activator [J]. Constr Build Mater, 2007, 21:1 342-1 350. 被引量:1
  • 4FRAIRE-LUNA P E. Composite system fluorgypsum-blast furnace slag-metakaolin, strength and microstructures [J]. Cem Concr Res, 2006, 36(6): 1 048-1055. 被引量:1
  • 5SINGH Manjit, GRAG Mridul. Activation of gypsum anhydrite-slag mixtures [J]. Cem Concr Res, 1995, 25(2): 332-338. 被引量:1
  • 6杨久俊,海然,杨久俊,吴科如.钙矾石的结构变异对膨胀水泥膨胀性的影响[J].无机材料学报,2003,18(1):136-142. 被引量:36