聚乙烯管道热熔接头无损检测技术研究进展

Research progress in non-destructive testing technology for polyethylene pipeline hot melt joints
下载PDF
导出
摘要 文中介绍了聚乙烯管热熔焊接原理与聚乙烯管热熔接头的常见缺陷,详细分析了聚乙烯燃气管热熔接头的几种无损检测方法:超声检测(常规超声波检测、超声相控阵检测、非线性超声波检测技术)、太赫兹检测、X射线检测和红外热成像等,讨论了各种无损检测技术理论及优缺点,总结了最新的研究进展。 This article introduces the principle of polyethylene pipe hot melt welding and common defects of polyethylene pipe hot melt joints.It analyzes in detail several non-destructive testing methods for polyethylene gas pipe hot melt joints:ultrasonic testing(conventional ultrasonic testing,ultrasonic phased array testing,nonlinear ultrasonic testing technology),terahertz testing,X-ray testing,and infrared thermal imaging.It discusses the theories and advantages and disadvantages of various non-destructive testing technologies,Summarized the latest research progress.
作者 方学锋 周楠 张伯君 于永亮 Fang Xuefeng;Zhou Nan;Zhang Bojun;Yu Yongliang(Nanjing Boiler&Pressure Vessel Inspection Institute,Nanjing 210019,China;Key Laboratory of the Oil&Gas Pipeline Inspection and Safety Technology for Jiangsu Province Market Regulation,Nanjing 210019,China)
出处 《炼油与化工》 CAS 2023年第3期11-14,共4页 Refining And Chemical Industry
基金 2021年江苏省市场监督管理局科技计划项目“聚乙烯PE管熔接接头非线性超声无损检测方法研究”(编号KJ21125072)。
关键词 聚乙烯 热熔接头 缺陷 无损检测 Polyethylene hot melt joint defect non-destructive testing