摘要
研究了采用浮选-重选联合工艺从内蒙古某低品位钨钼矿石中分选钼精矿及钨精矿。结果表明:钼精矿回收率88.89%,钼品位50.24%;钨精矿回收率81.87%,钨品位52.88%,分选效果较好。
Molybdenite and wolframite is separated from a low-grade tungsten-molybdenum ore from Inner Mongolia by a combined processing flowsheet of flotation-gravity concentration.The results show that the molybdenum concentrate with molybdenum of 50.24%at recovery of 88.89%and tungsten concentrate with tungsten of 52.88%at recovery of 81.87%are obtained,respectively.The mineral processing effect is good.
作者
刘永祥
曹辉
韩晓阳
廖璐
LIU Yongxiang;CAO Hui;HAN Xiaoyang;LIAO Lu(Inner Mongolia Mining Exploitation Co.Ltd.,Hohhot 010010,China;Inner Mongolia Minerals Experiment Research Institute,Hohhot 010031,China)
出处
《湿法冶金》
CAS
北大核心
2020年第6期468-472,共5页
Hydrometallurgy of China
关键词
钨钼矿石
钼精矿
钨精矿
分选
tungsten-molybdenum ore
molybdenum concentrate
tungsten concentrate
separation