1#1880 m^3高炉炉凉恢复实践

Practice of Furnace Cooling and Recovery for 1#1880m^3 BF
下载PDF
导出
摘要 介绍了型钢炼铁厂1#1880 m^3高炉无计划停煤的经过、停煤前的炉况基础、恢复过程及采取的措施,特别是对补煤的数量进行了计算,并对炉况恢复经验进行了归纳总结,提出了高炉炉凉的处理思路。 For 1#1880m^3 blast furnace in the Section Steel Ironmaking Plant,this paper introduced the process of unplanned stopping coal injection,the basis of furnace condition before stopping coal injection,the recovery process and the measures taken,especially calculated the coal replenishment amount,and further summarized the recovery experience of furnace condition,put forward the treatment ideas for blast furnace cooling.
作者 朱明琦 Zhu Mingqi(The Ironmaking Plant)
机构地区 型钢炼铁厂
出处 《莱钢科技》 2020年第3期37-39,42,共4页 Laigang Science & Technology
关键词 高炉 停煤 炉况 补煤量 blast furnace stopping coal injection furnace condition coal supplement amount