期刊文献+

云南某低品位磁铁矿选矿试验研究 被引量:7

Beneficiation Technology for Lean Magnetite Ore from Yunnan Province
下载PDF
导出
摘要 对云南某原矿TFe品位22.35%、磁性铁含量15.58%的贫磁铁矿进行了选矿试验研究。经过不同粒度预选试验和多流程对比试验,开发出了适合该矿的选矿工艺流程,采用粗粒预选-磨矿-弱磁选-重选-再磨-弱磁选流程,取得了精矿产率23.89%、TFe品位65.70%、回收率70.28%的指标。 Experimental study was carried out to beneficiate a lean magnetite ore from Yunan Province with TFe grade of 22.35% and magnetic iron(mFe) content of 15.58%. Based on preconcentration tests with varied feed size and contrast tests of multiple processes, a suitable dressing flowsheet is proposed. It is shown that a flowsheet consisting of sequentially coarse fraction preconcentration, grinding, low intensity magnetic separation(LIMS), gravity separation, regrinding and LIMS processes, can produce an iron concentrate grading 65.70% TFe at 70.28% recovery with the yield of 23.89%.
作者 李煊生 罗良飞 LI Xuan-sheng;LUO Liang-fei(Lan County Mining Co Ltd, Taiyuan Iron & Steel ( Group) Co Ltd, Lan County 030027, Shanxi, China;Changsha Research Institute of Mining & Metallurgy Co Ltd, Changsha 410012, Hunan , China)
出处 《矿冶工程》 CAS CSCD 北大核心 2019年第4期68-71,共4页 Mining and Metallurgical Engineering
关键词 磁铁矿 磁选 重选 预选 磨矿 magnetite magnetic separation gravity separation preconcentration grinding
  • 相关文献

参考文献4

二级参考文献8

共引文献15

同被引文献51

引证文献7

二级引证文献13

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部