三元正极材料LiNi_(0.5)Co_(0.2)Mn_(0.3)O_2具有能量密度大、比容量高、成本低等优点,已基本实现产业化。但该材料的容量保持率低和热稳定性能差阻碍了其全面快速的发展。综述了制备工艺的优化、掺杂和包覆等改性方法对三元正极材料性能的影响,重点介绍了热电化学和数值模拟的研究现状和应用。
LiNi0.5Co0.2Mn0.3O2cathode material with enormous energy density,higher capacity and lower cost has basically realized industrialization.But its comprehensive and rapid development are hampered attributed to its low retention rate and poor thermal stability.In this paper,the effects of preparation process optimization,doping and coating methods on the properties of ternary cathode materials are reviewed.The research status and application of thermoelectrochemistry and numerical simulation are introduced.
作者
宋刘斌
李新宇
肖忠良
曹忠
朱华丽
SONG Liubin;LI Xinyu;XIAO Zhongliang;CAO Zhong;ZHU Huali(School of Chemistry and Biological Engineering, Changsha University of Science and Technology, Changsha 410004, China;School of Physics and Electronic Engineering, Changsha University of Science and Technology, Changsha 410004,China)
出处
《功能材料》
EI
CAS
CSCD
北大核心
2017年第12期12023-12029,12035,共8页
Journal of Functional Materials
基金
国家自然科学基金资助项目(21501015
51604042
21545010
31527803)
中国科学院环境监测STS资助项目(KFJ-SW-STS-173)
湖南省自然科学基金资助项目(2016JJ3007)
湖南省科技计划资助项目(2015GK1046)