摘要
因氧化锌工艺特殊,因要稳定氧化锌的性质,须严格控制其中硫的含量,而因其工艺复杂,含量复杂,所以需要一种稳定快速的测留方法。
Because of the special process of Zinc Oxide,the sulfur content must be strictly controlled in order to stabilize the properties of Zinc Oxide. Because of its complex process and complex content,a stable and rapid meth Keywords: Zinc Oxide titration iodin method neutralization method high temperature combustion furnaceod of retention is needed.
作者
徐晓凤
Xu Xiaofeng(Guangdong Mineral Resources Research Institute Key Laboratory of Radioactive and Rare Scattered Minerals Comprehensive Utilization,Ministry and Land and Resources,Shaoguan 512026,China)
出处
《山东化工》
CAS
2018年第13期76-77,共2页
Shandong Chemical Industry
关键词
氧化锌
滴定法
碘量法
中和法
高温燃烧炉
Zinc oxide
titration method
iodometry
acid-base titration