船舶折角型节点的疲劳裂纹扩展计算(英文) 被引量:1

Fatigue Crack Growth Calculation of a Surface Crack in a Ship Angular Joint
下载PDF
导出
摘要 文章以船舶折角型节点为研究对象,运用有限元软件WALCS和PATRAN分别预报某船的水动力响应和结构热点应力响应。为避免计算表面裂纹应力强度因子时需要在PATRAN有限元模型中疲劳热点区域采用体单元建模,文中提出了一种计算波浪载荷下船海结构物三维表面裂纹应力强度因子而无需在PATRAN中建立体模型的方法,并通过与广泛认可的经验公式对比验证其精度。将此方法应用于该船船舯底边舱折角处表面裂纹应力强度因子计算,计算并总结出波浪载荷下该类节点处表面裂纹应力强度因子的无量纲计算经验公式。应用一种基于谱分析构建结构疲劳载荷谱的方法,结合单一曲线模型对该节点进行裂纹扩展计算。计算结果表明:该船船舯底边舱折角疲劳寿命不满足设计要求,建议对节点进行改进。 An angular joint in a container is taken as the research object. Hydrodynamic response and structural hot spot stress response of a container were forecasted by using the finite element software WALCS and PATRAN respectively. In order to avoid using 3D solid element in the hot spot area in PATRAN finite element model for calculating the stress intensity factor(SIF) of a surface crack, a SIF calculation method for surface cracks in ship structures under wave loads was proposed. The accuracy of the proposed method was validated by comparing the calculated results with those of widely accepted empirical formulas. Then, the method was applied to an angular joint in the bottom at the midship. SIFs of surface cracks with different sizes in the joint under the wave induced pressure were calculated and dimensionless empirical formulas were summarized. The fatigue load spectrums were generated by using a method based on spectrum analysis. Fatigue crack growth was calculated by using the unique crack growth rate curve model. Calculation results showed that the discussed hot spot did not meet the requirement of design life and further modification will be needed.
出处 《船舶力学》 EI CSCD 北大核心 2017年第9期1114-1127,共14页 Journal of Ship Mechanics
基金 Supported by National Natural Science Foundation of China(Project No.51279102) project ‘Study on the fatigue strength of Thick High Tensile Steel plate ’ financially supported by China Classification Society~~
关键词 波浪载荷 折角型节点 表面裂纹 应力强度因子 单一曲线模型 wave load angular type joint surface crack stress intensity factor unique curve model
  • 相关文献

参考文献3

二级参考文献50

  • 1邱强.船舶随机波浪载荷的理性预报方法[J].中国造船,2007,48(2):37-44. 被引量:5
  • 2Suresh S,Ritchie R O.On the influence of environment on the load ratio dependence of fatigue thresholds in pressure vessel steel[J].Engng Fracmre Mech.,1983,18:785-800. 被引量:1
  • 3Chang T,Guo W.Effects of strain hardening and stress state on fatigue crack closure[J].Int J Fatigue,1999,21:881-888. 被引量:1
  • 4BS7910.Guide on methods for assessing the acceptability of flaws in structures[M].British Standards Institution,1999. 被引量:1
  • 5King R.A review of fatigue crock growth rates in air and seawater[M].HSE Report OTH 511,London,Health & Safety Executive Books,1998:ISBN 0717621437. 被引量:1
  • 6Tsukuda H,Ogiyama H,Shiraishi T.Fatigue crack growth and closure at high stress ratios[J].Fatigue Fract Eng Mater Struct.,1995,18:503-514. 被引量:1
  • 7Tan J M L,Fitzpatrick M E,Edwards L.Stress intensity factors for through-thickness cracks in a wide plate:Derivation and application to arbitrary weld residual stress fields[J].Eng.Frac.Mech.,2007,74:2030-2054. 被引量:1
  • 8Huang X P,Moan T.Improved modeling of the effect of R-ratio on crack growth rate[J].Int.J Fatigue,2007,29:591-602. 被引量:1
  • 9Huang Xiaoping.Fatigue crack growth rote recommended in BS7910 and a unique crack growth rote curve under different load ratios[C]//ASME PVP 2007/CREEP 8 Conference July 22-26,2007.San Antonio,Texas,USA,2007. 被引量:1
  • 10Huang X P,Moan T,Cui W C.An engineering model of fatigue crack growth under variable amplitude loading[J].Int.J Fatigue,2008,30:2-10. 被引量:1

共引文献28

同被引文献4

引证文献1

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部