期刊文献+

山东某焙烧氰化尾渣综合回收工艺研究 被引量:6

Study on comprehensive recovery of roasting cyanidation residue in Shandong Province
下载PDF
导出
摘要 针对山东某焙烧氰化尾渣的性质,采用高温氯化焙烧工艺对其进行了综合回收试验研究。结果表明:在氯化钙添加量7%、焙烧温度1 100℃、焙烧时间2 h的工艺条件下,有价金属Au、Ag、Cu、Pb、Zn的挥发率分别达到97.52%、71.78%、85.92%、98.59%、93.81%,指标较好。同时,根据试验结果提出了尾渣综合回收有价金属的工艺流程,为后续研究奠定了基础。 High-temperature chloridizing roasting process has been carried out for experimental study on comprehensive recovery of some roasting cyanidation residue from Shandong according to its properties. The results show that under the optimum parameters,that is Ca Cl2 addition 7 %,roasting temperature 1 100 ℃ and roasting time 2 h,the volatilization rate of main valuable metals including Au,Ag,Cu,Pb and Zn can reach 97. 52 %,71. 78 %,85. 92 %,98. 59 % and 93. 81 % respectively. Based on the results,the process of comprehensive recovery of valuable metals from roasting cyanidation residue was proposed,which pointed out the direction for subsequent research.
出处 《黄金》 CAS 2017年第2期50-53,57,共5页 Gold
基金 国家高技术研究发展计划(863计划)项目(2011AA06A104)
关键词 高温氯化焙烧 焙烧氰化尾渣 综合回收 有价金属 挥发率 high-temperature chloridizing roasting roasting cyanidation residue comprehensive recovery valuable metal volatilization rate
  • 相关文献

参考文献7

二级参考文献35

共引文献92

同被引文献53

引证文献6

二级引证文献17

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部