针对目前莱钢生产的履带钢腿端划伤问题,研究现有精轧机导卫装置,通过改进入口和出口导卫装置,解决了履带钢腿端划伤问题,提高产品表面质量,提高生产效率。
According to the scratches on the top- leg of track steel produced by Laiwu steel in the current,the paper studies on the guiding equipment of finishing mill,reformes the entry guides and exit guides,solves the problem of the scratches on the top- leg of track steel,improves the surface quality and production efficiency.