摘要 研究了采用回转短窑对硫铁矿烧渣进行焙烧以回收有价金属的方法,考察了不同的工艺条件对硫铁矿烧渣焙烧的影响。研究结果表明:在还原温度在1 250℃下、还原时间为60min下,硫铁矿烧渣得到充分的还原。金、银、铜、铅、锌的挥发率中试分别达到93.26%,82.20%,82.55%,88.53%和83.48%,此时球团的硬度可以达到2 100N。 The roasting method was used to recover valuable metals from pyrites cinder in rotary kiln, and the influences of different process conditions on roasting pyrite cinder were examined. The results show that the pyrite cinder can be fully reduced under the conditions of reaction temperature at 400℃ and reaction time for 60 minutes. The volatilizing rates of gold, silver, copper, lead and zinc in pilot scale experiment can reach 93.26%, 82.20%, 82.55%, 88. 53% and 83.48%, respectively. Hardness of the pellets can reach 2100 N at this time.
作者 范增
出处 《有色矿冶》 2015年第5期32-34,共3页 Non-Ferrous Mining and Metallurgy
关键词 硫精矿烧渣 球团硬度 挥发率 还原温度 sulfur concentrate cinder pellets hardness reduction temperature the volatilization rate
  • 相关文献

参考文献7

  • 1任贵义.炼铁学[M].北京:冶金工业出版社,2004. 被引量:4
  • 2田彦文,翟秀静,刘奎仁编..冶金物理化学简明教程[M].北京:化学工业出版社,2007:293.
  • 3邱竹贤主编..有色金属冶金学[M].北京:冶金工业出版社,1988:424.
  • 4李洪桂主编..冶金原理[M].北京:科学出版社,2005:384.
  • 5彭正英,李生元,赵克智.用离析浮选从栖霞山黄铁矿烧渣中提取银金的试验研究[J].江苏冶金,1982(4):14-20. 被引量:3
  • 6黄海辉,王云,袁朝新,李云.从提金渣中回收金银[J].有色金属(冶炼部分),2011(10):37-39. 被引量:19
  • 7丁剑,孙建伟,钱鹏,潘占开,叶树峰,李青春,王彩霞,陈运法.氯化焙烧回收高铁硫酸烧渣中有价金属的实验研究[J].计算机与应用化学,2012,29(3):255-261. 被引量:16

二级参考文献13

共引文献33

同被引文献27

引证文献2

二级引证文献3

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部