摘要 鞍钢5号高炉燃料比平均在590 kg/t以上,采用提高焦丁用量并与矿石混装技术措施后燃料比降低。实验室测试和模拟计算结果表明,随着焦丁用量提高,矿石在块状带透气性得到改善,尤其是软融带区域透气性改善显著。鞍钢5号高炉试验结果表明,当粒度为10~30 mm小粒度焦炭与矿石混装入炉,焦丁比提高到60~80 kg/t时,降低高炉燃料消耗效果显著,焦丁与焦炭置换比可以保持在1.0以上。 The fuel ratio of No.5 BF in Angang is more than 590 kg/ton on the average, while the fuel ratio of the BF is reduced by taking such measures as increasing the adding amount of nut coke and applying the technology of mixed charging of nut coke and ore. The test results in laboratory and the simulating calculation results show that the permeability of ore in lump zone is improved, particularly the permeability of ore in cohesive zone is improved remarkably with increasing adding amount of nut coke. So the test for No.5 BF of Angang shows that the effect of decreasing the fuel consumption in BF is remarkable and the replacement ratio between nut coke and coke can be kept over 1.0 as fine particle coke with the size from 10 mm to 30 mm is charged into the BF together with ore and the charging ratio of nut coke is increased to the range from 60kg/t to 80 kg/t.
出处 《鞍钢技术》 CAS 2015年第1期18-22,共5页 Angang Technology
关键词 高炉 焦丁 混装 燃料比 透气性 blast furnace nut coke mixed charging fuel ratio permeability
  • 相关文献

参考文献6

二级参考文献10

  • 1李家新,糜克勤.混装焦丁时的焦炭热强度及适宜加入量[J].炼铁,1994,13(6):53-54. 被引量:3
  • 2徐万仁,张龙来,张永忠,李有庆.高小块焦比操作对高炉透气性和煤气流分布的影响[J].炼铁,2005,24(5):27-30. 被引量:15
  • 3武川正博.大量使用小块焦实现高利用系数低燃料比稳定操作.材料&プロヤス,1999,(12):92~94. 被引量:1
  • 4Hans Bodl Luengen, Michael Peters, Peter Sehmole. Ironmaking in West European [ C ]//AISTech 2011 Proceedings. USA: The Association of Iron & Steel Technology, 2001:387 -400. 被引量:1
  • 5Shiro Watakabe, Kanji Takeda, Hirobumi Nishimura, et al. Development of High Ratio Coke Mixed Charging Technique to the Blast Furnace [ J ]. ISIJ International, 2006,46 (4) :513 - 522. 被引量:1
  • 6Elsaved A, Mousa, Alexander Babich, et al. Effect of Nut Coke- slnter Mixture on the Blast Furnace Performance [ J ]. ISIJ International, 2011,51 (3) :350 - 358. 被引量:1
  • 7Muneyoshi Sawayama, Kazuya Miyagawa, Kentaro Nozawa,et al. Low Coke Rate Operation of Blast Furnace by Controlling Size of Coke Mixed into Ore Layer [ C ]//Proceeding of the 5th International Congress on the Science and Technology of Ironmaking. China :The Chinese Society for Metals, 2009:663-667. 被引量:1
  • 8Takeshi Sato, Shiro Watakabe, Kanji Takeda. Burden distribution control for high perfolrnance of blast furnace operation at JFE steel [C ]//36th MeMASTER University Symposium on Iron and Steelmaking. Canada :McMASTER University,2008 : 129 - 157. 被引量:1
  • 9张寿荣,傅连春,杨佳龙.2011年欧洲炼铁技术考察报告[J].炼铁,2011,30(6):52-57. 被引量:1
  • 10刁日升,刘树芳,杨志远.攀钢高炉焦丁混装入炉生产实践[J].钢铁钒钛,2000,21(1):45-49. 被引量:7

共引文献13

同被引文献22

引证文献3

二级引证文献8

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部