摘要 山东钢铁股份有限公司莱芜分公司通过控制电炉终点碳在0.12%-0.25%;LF精炼渣碱度B=3.0;VD炉真空度小于67Pa保持时间大于25min;连铸采用氩气密封水口保护浇铸;过热度控制在(20±5)℃;结晶器电磁搅拌电流I=200A、频率F=3Hz;同时采用动态二冷配水技术,成功开发的4130连铸圆坯[O]≤20ppm,[N]≤80ppm,[H]≤2ppm;低倍组织≤1.0级;锻件夹杂物A、B≤1.0级,C、D、Ds≤0.5级;锻件超声波探伤≥3级;圆坯的尺寸、外形以及碳偏析等各项指标均满足了石油套管连接件用钢技术要求。 Shandong iron and steel Limited by Share Ltd Laiwu branch developed the 350mm diameter 4130 round billet continuous casting, by using the following technical measures: control the end point carbon of electric furnace in 0.12%-0.25%; LF refining slag basicity B=3.0; Keep the time more than 25 minutes, when the vacuum degree of VD furnace is less than 67 Pa; Using argon sealing nozzle protective casting; control the superheat of molten steel in (20 + 5)~C; control the electromagnetic stirring of crystallizer/--200 A, F=3 Hz; using the Two dynamic cooling section water distribution technique etc. The product technical indicators, such as [O] ≤ 20 ppm,[N] ≤80 ppm,[H] ≤ 2 ppm, Maerostrueture level ≤ 1.0, A&B class of non metallic inclusions ≤ 1.0, C&D&Ds class of non metallic inclusions ≤0.5, The size, shape and carbon segregation of round billet etc. all meet the quality requirements of oil casing connector user.
作者 时振明
出处 《冶金标准化与质量》 2014年第6期14-18,共5页 Metallurgical Standardization & Quality
关键词 4130钢 石油套管连接件 圆坯 steel 4130 oil casing connector round billet
  • 相关文献

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部