摘要
为了最大限度地利用包钢高炉矿渣微粉和粉煤灰,尽可能地减少熟料用量来配制325复合硅酸盐水泥,对复合水泥的配合比进行试验研究,得出当水渣的掺量小于37%,采用石膏、熟料、水渣、粉煤灰4种原料一起混磨配制复合水泥的各项指标均能达到325复合水泥的标准要求。
In order to farthest utilize the fly ash and micro powder of blast furnace slag in Baotou Steel as well as reduce the consumption of chamotte to produce 325 composite portland cement,the proportioning is tested and studied. The results show that when the amount of grain slag is smaller than 37%,all the indexes of composite cement produced with gypsum,chamotte,grain slag and fly ash could meet the requirements of standard for 325 composite cement.
出处
《包钢科技》
2014年第5期86-88,共3页
Science & Technology of Baotou Steel