摘要
采用蒸汽养护技术,通过试验研究了以建筑淤土为主要原材料,制备免烧陶粒的可行性,对试验所用其他材料及方法作了介绍,研究结果表明,以建筑淤土为主要组成材料,并辅以水泥、石灰石和石膏可以制备出免烧陶粒。
The paper adopts the steam curing technique, researches the architectural soft soil as the main raw materials by the tests and the feasibility for the unbaked ceremsite, introduces other materials and methods in the tests, and proves by the research results that ceremsite can be made with the main materials of the architectural soft soil and cement, limestone and gypsum unbaked.
出处
《山西建筑》
2014年第28期116-117,共2页
Shanxi Architecture
基金
宁波市择优委托项目(项目编号:2011C11009)
国家级大学生创新创业训练计划项目(项目编号:201313022013)
宁波市农村与社会发展领域科技计划(项目编号:51108415)
关键词
建筑淤土
免烧陶粒
筒压强度
吸水率
architectural soft soil, unbaked ceremsite, cylinder pressure strength, water absorption