加氢裂化热高分油管线弯头开裂分析

Analysis of the Elbow Cracking on High-temperature Separation Pipeline of Hydrocracker
下载PDF
导出
摘要 对国产加氢裂化热高分油管线的弯头开裂原因进行了分析 ,对预防连多硫酸腐蚀提出了相应的防范措施 :选用碳含量 <0 .0 3 %并含有稳定化元素Ti、Nb的奥氏体不锈钢或双相钢 ;控制焊缝硬度不大于HB2 0 0并焊后热处理 ;12CrMo和 15CrMo耐应力腐蚀性能好 ; The cracking of the elbow on the high-temperature separation pipeline of the domestic hydrocracker was analyzed. The corresponding protection measures against polythionic acid corrosion were presented: ie selection of austenic steel or duplex steel with carbon less than 0.03% and stablizing elements like Ti and Nb and the hardness of the welds controlled at no greater than HB200 and implementation of heat treatment. 12CrMo and 15CrMo had good performance against stress corrosion. The equipment should be cleaned and neutralized by caustics immediately after shutdown.
出处 《石油化工腐蚀与防护》 CAS 2002年第1期38-41,共4页 Corrosion & Protection In Petrochemical Industry
关键词 加氢裂化 热高分油管线 弯头开裂 炼油 奥氏体不锈钢 连多硫酸 腐蚀 austenic stainless steel, polythionic acid, corrosion
  • 相关文献

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部