摘要
新疆某铅锌矿铅锌含量较低,为了综合利用资源,采用优先浮选流程进行选矿试验研究,闭路试验获得了含铅63.10%、含锌4.82%、铅回收率78.43%的铅精矿和含锌50.43%、含铅1.03%、锌回收率86.49%的锌精矿。
It is a low-grade lead-zinc ore of Xinjiang, for the purpose of comprehensive utilization of these resources, selective flotation process was adopted to research on mineral processing of this low grade lead-zinc ore of Xinjiang, finally the lead concentrate containing 63.10% Pb and 4.82% Pb and zinc concentrate containing 50.43% Zn and 1.03% Pb were obtained by the closed-circuit, at recoveries of 78.43% Pb and 86.49% Zn.
出处
《有色金属(选矿部分)》
CAS
北大核心
2014年第2期9-11,共3页
Nonferrous Metals(Mineral Processing Section)
关键词
硫化矿
铅锌矿
优先浮选
sulphide ore
lead-zinc ore
selective flotation