摘要
Two kinds of aliphatic alternating polyesteramide prepolymers were prepared through melt polycondensation from N,N'-bis(2-hydroxyethyl)-adipamide and adipic acid or sebacic acid. Chain extension of them was conducted with 2,2'-(1,4- phenylene)-bis(2-oxazoline) and adipoyl biscaprolactamate as combined chain extenders. The chain extended polyesteramides (ExtPEAs) were characterized by IR, 1H-NMR, differential scanning calorimetry, thermogravimetric analysis, wide angle X-ray scattering, tensile test and enzymatic degradation. The results showed that the ExtPEA(4,m)s were mainly constituted with the diester adipamide alternating units. ExtPEA(4,4) and ExtPEA(4,8) had Tm of 83.8℃ and 85.8℃ and initial decomposition temperature above 310.0℃. They crystallized similarly as Nylon-66 did and were flexible thermoplastic materials with tensile strength up to 25.64 MPa and strain at break up to 737%.
Two kinds of aliphatic alternating polyesteramide prepolymers were prepared through melt polycondensation from N,N'-bis(2-hydroxyethyl)-adipamide and adipic acid or sebacic acid. Chain extension of them was conducted with 2,2'-(1,4- phenylene)-bis(2-oxazoline) and adipoyl biscaprolactamate as combined chain extenders. The chain extended polyesteramides (ExtPEAs) were characterized by IR, 1H-NMR, differential scanning calorimetry, thermogravimetric analysis, wide angle X-ray scattering, tensile test and enzymatic degradation. The results showed that the ExtPEA(4,m)s were mainly constituted with the diester adipamide alternating units. ExtPEA(4,4) and ExtPEA(4,8) had Tm of 83.8℃ and 85.8℃ and initial decomposition temperature above 310.0℃. They crystallized similarly as Nylon-66 did and were flexible thermoplastic materials with tensile strength up to 25.64 MPa and strain at break up to 737%.
基金
financially supported by the National Natural Science Foundation of China (Nos.50873013 and 21244006)