摘要
用 XRD法研究配料粒度、烧结温度及陈化处理诸因素对生成尖晶石相 Zn Cr2 O4数量的影响 ,结果表明 ,在 80 0~ 110 0℃间 ,原料的陈化处理可促进尖晶石相 Zn Cr2 O4的生成。
ELECTRONIC COMPONENTS & MATERIALS (China), Vol 19, No 3, P 7 8 (Jun 2000) In Chinese The effects of graininess, sintering temperature and aging treatment on the generation of spinel ZnCr 2O 4 are investigated by means of XRD. The factors have an influence over the quantity of spinel. ZnCr 2O 4 generated. At 800~1 100℃, aging treatment is helpful to the generation of spinel ZnCr 2O 4. (4 refs.)