摘要
以质量分数35%的过氧化氢水溶液及冰醋酸为氧化剂,采用超声氧化消解的方法从含铼离子液体中分离回收铼。当高铼酸盐离子液体为2.5mmol时,超声氧化消解含铼离子液体的适宜条件为质量分数35%的H2O2水溶液为25mmol、冰醋酸为15mmol时,50℃条件下超声氧化24h,使用氨水将溶液pH调至9~10。经回收得到铼化合物的最佳回收率为69.07%。实验结果表明,经以上过程得到铼产品为高铼酸铵,粗产品纯度为99%。
The ultrasonic oxidation digestion method was used for the separation and recovery of rhenium from the rhenium containing ionic liquids, using 35% of hydrogen peroxide solution and acetic acid as the oxidizing agent. When the concentration of the perrhenate based ionic liquid is 2. 5 mmol, 35% the H2O2 aqueous solution was 25 mmol and the acetic acid was 15 retool, keep the ultrasonic oxidation under the conditions of 50℃ for 24 h, and then the pH value was adjusted to 9 to 10 with ammolonia solution, 69. 07% of rhenium compound can be recovered from the ILs. It has been proved that the recycled rhenium product is ammolonium perrhenate, and the purity is about 99%.
出处
《石油化工高等学校学报》
CAS
2012年第6期10-13,共4页
Journal of Petrochemical Universities
基金
国家自然科学基金资助项目(21071073
21101085)
辽宁省自然科学基金资助项目(201102116)
关键词
超声氧化
分离回收
消解
铼
离子液体
Ultrasonic oxidation
Separation and recovery
Digestion
Rhenium
Ionic liquid