摘要 为了适应TFT-LCD小型化与窄边框化以及在面板布线精细化的趋势,提高工艺设计富裕量以及增加面板的实际利用率,研究了通过改变钝化层(PVX)的沉积工艺来减小液晶面板阵列工艺中连接像素电极与漏极的过孔(VIA)尺寸的方案,通过设计实验考察了影响过孔大小的钝化层的主要影响因素(黑点、倒角、顶层钝化层沉积厚度,顶层钝化层沉积压力),得出了在不改变原有刻蚀方式基础之上使过孔的尺寸降低20%~30%的优化方案,并对其进行了电学性能评价(Ion:开态电流、Ioff:关态电流、Vth:阈值电压、Mobility:迁移率),从而获得了较佳的减小过孔尺寸的方案,提高了产品品质。 In the trend of miniaturization narrow frame and fine wiring structure,the TFT-LCD tends to developing for large margin of design and high real substrate utilization rate.The passivation layer deposit parameters were changed to decrease the size of via hole which connected the pixel electrode and drain electrode were studied.Through the experiments design of changing main parameters to minimize via hole of passivation layer(haze,undercut,Top-PVX deposit thickness,Top-PVX deposit pressure),a solution to minimize the via hole about 20%~30% without changing the etch conditions was found.The electronic parameter measurement was evaluated(Ion,Ioff,Vth,Mobility) and finally one better solution to minimize via hole size was obtained.Therefore,the products quality was improved also.
出处 《液晶与显示》 CAS CSCD 北大核心 2012年第4期493-498,共6页 Chinese Journal of Liquid Crystals and Displays
基金 京东方研发基金(10SVHM)
关键词 钝化层 刻蚀 过孔 passivation layer etch VIA hole
  • 相关文献

参考文献9

二级参考文献32

  • 1唐元洪.等离子增强型化学气相淀积氮化硅的淀积[J].湖南大学学报(自然科学版),1996,23(1):42-44. 被引量:3
  • 2金奉柱,崔瑩石,劉聖烈,張炳鉉,柳在一,李禹奉,李貞烈.利用CF_4等离子体制作高开口率TFT-LCD(英文)[J].液晶与显示,2006,21(5):409-413. 被引量:3
  • 3丁晖,徐重阳,邹雪城,张少强.PECVD a-Si:H薄膜对TFT有源矩阵性能的影响及其淀积工艺研究[J].光电子技术,1997,17(1):28-32. 被引量:7
  • 4MacDonald W A, Looney M K, Mackerron D, et al. Latest advances in substrate for flexible electronics [J]. J. SID, 2007, 15(12) :1075-1083. 被引量:1
  • 5Gleskova H, Wagner S,Suo Z. a-Si= H TFT made on polyimide foil by PECVD at 150 ℃ [J]. Flat Panel Display Material, 1998, 508:73-78. 被引量:1
  • 6Raupp G B, Shawn M O, Moyer C,et al. Low-temperature amorphous-silicon backplane technology development for flexible displays[J]. J. SID, 2007, 15(7) 1445-454. 被引量:1
  • 7Kim J H, Oh E Y, Ahn B C, et al. Performance improvement of a-Si: H TFT with SiO2 insulator by N2 plasma treatment[J]. Appl. Phys. Lett., 1994, 64(6):775-776. 被引量:1
  • 8Gallezot J D, Martin S, Kanicki J. Photosensitivity of a-Si: H TFT [C]//Asia Display/IDW01, Nagoya, Japan: SID, 2001:407-410. 被引量:1
  • 9Hori H, Suzuki K. ColorEkisho Display [M]. Beijing: Science Press, 2003:94-141. 被引量:1
  • 10Chang Tashan, Chang Tingehang, Liu Potsun, et al. Improvement of hydrogrnated amophous-silicon TFT perfor- mances with low-k siloxane-based hydrogen silsesquioxane (HSQ) Passivation Layer [J]. IEEE Electron Device Letters, 2006, 27(11).. 902-904. 被引量:1

共引文献37

同被引文献34

引证文献4

二级引证文献13

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部