摘要 目的 探讨金 瓷修复体瓷裂或瓷崩的原因。方法 随机选择 16例前牙和前磨牙区因瓷裂或瓷崩而导致失败的病例 ,记录修复体损坏的部位 ,分析产生失败的原因。结果 瓷裂或瓷崩发生在切缘的病例数为 10例 (占 6 2 .5 % ) ,发生在连接体部位有 4例 (占 2 5 % ) ,发生在其他部位的有 2例 (占 12 .5 % )。结论 金 瓷修复体损坏与临床设计、牙体制备及技术室制作有密切的关系。 Objective To investigate the reasons of fracture or exfoliation of metal porcelain prosthesis. Methods 16 cases with fracture or exfoliation on the area of anterior teeth and premolar were selected, the damage's parts of prosthesis were recorded, and the causes of failure were analyzed. Results 10 cases(62.5%) on incisal margin, 4 cases(25%)on the connector and 2 cases(12.5%)on the other parts were found. Conclusion Damages of metal porcelain may be related to clinical design, preparation and manufacture in technique room.
作者 邓汉龙
出处 《口腔材料器械杂志》 2000年第2期75-77,共3页 Chinese Journal of Dental Materials and Devices
关键词 金-瓷修复体 瓷裂 瓷崩 metal porcelain prosthesis fracture exfoliation
  • 相关文献

参考文献7

二级参考文献9

共引文献301

同被引文献31

  • 1贾建设.修复体金瓷结合强度的研究进展[J].河南职工医学院学报,2005,17(2):126-128. 被引量:2
  • 2华瑛.材料的热膨胀性能及其影响因素[J].上海钢研,2005(2):60-63. 被引量:26
  • 3蒋永林 高法章.460例烤瓷熔附金属修复体疗效观察[J].上海口腔医学,1997,:97-97. 被引量:16
  • 4Rungan D A. Fluid absorbency ofret Rection Cords after Soaking in aluminum Chloride Solution. J ProthetDent, 1988,60:676. 被引量:1
  • 5Bagby M, Marshall S J, Marshall GW Jr. Metal ceramic compati-bility: A review of the literature[J]. J Prosthet Dent, 1990, 63 (1): 21-25. 被引量:1
  • 6Zinelis S, Tsetsekou A, Papadopoulos T. Thermal expansion and microstructural analysis of experimental metal-ceramic titanium alloys[J]. J Prosthet Dent, 2003, 90(4):332-338. 被引量:1
  • 7Coffey JP, Anusavice K J, DeHoff PH, et al. Influence of contrac- tion mismatch and cooling rate on flexural failure of PFM systems [J]. J Dent Res, 1988, 67(1):61-65. 被引量:1
  • 8DeHoff PH, Anusavice KJ. Viscoelastic stress analysis of thermally compatible and incompatible metal-ceramic systems[J]. Dent Mater, 1998, 14 (4) : 237-245. 被引量:1
  • 9Yilmaz H, Dinner C. Comparison of the bond compatibility of tita- nium and an NiCr alloy to dental porcelain[J]. J Dent, 1999, 27 (3) : 215-222. 被引量:1
  • 10Anusavice K J, Dehoff PH, Gray A, et al. Delayed crack develop- ment in porcelain due to incompatibility stress[J]. J Dent Res, 1988, 67(8) : 1086-1091. 被引量:1

引证文献6

二级引证文献17

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部