摘要
通过水解TiCl_4制备了锐钛矿结构TiO_2纳米粒子,并用时间分辨荧光光谱研究了5(6)CFL(5(6)-Carboxyfluorescein,简称5(6)CFL)染料敏化TiO_2纳米粒子体系的光致电子转移动力学.5(6)CFL染料敏化TiO_2纳米粒子能形成电荷转移复合物,这归因于染料分子的激发电子态波函数Ψ(D*)与电荷分离态波函数Ψ(D^++e^-)之间的耦合作用.当激发5(6)CFL染料敏化TiO_2纳米粒子体系时,电子以两种不同方式注入TiO_2纳米粒子导带:第一,通过5(6)CFL染料分子的激发态注入;第二,从电荷转移复合物(5(6)CFL/TiO2)直接注入.时间分辨荧光光谱表明,在水溶液中纯5(6)CFL染料的荧光以寿命为Τ_1=41 ps(74.4%)和Τ_2=3.22 ns(25.6%)的双e指数衰减,而5(6)CFL染料敏化TiO_2纳米粒子体系的荧光分别以时间常数为Τ_1=44 ps(90.4%),Τ_2=478 ps(8.6%)和Τ_3=2.41 ns(1.0%)的三e指数衰减.本文的研究工作能够为染料敏化太阳能电池的光致电子转移机理提供有价值的参考.
Anatased TiO2 nanoparticles were prepared by controlling hydrolysis of the TiCl4.Time-resolved fluorescence experiments were carried out to study the photo-induced electron transfer dynamics in the system of the 5(6)CFL dye-sensitized TiO2 nanoparticles.For the aboved system,the formation of the charge transfer complex is attributed to the coupling interaction between the wave functions of the excited electronic state of the dye(Ψ(D~*)) and the charge separated state(Ψ(D~++e^-)).On excitation of 5(6)CFL dyesensitized TiO2 nanoparticle system.The injection of electrons into the conduction band of TiO2 nanoparticles takes place in two different ways:through the excited state of the 5(6)CFL dye and through direct injection from the charge transfer complex.The time-resolved fluorescence experimental results indicate that the free 5(6)CFL dye in water has double-exponential decay with lifetimesτ1 41 ps(74.4%) andτ2= 3.22 ns(25.6%).However,5(6)CFL dye-sensitized TiO2 nanoparticles have triple-exponential decay with lifetimes ofτ1= 44 ps(90.4%),τ2= 478 ps(8.6%) andτ3= 2.41 ns(1.0%).Our research will provide a valuable reference for the mechanism of dye-sensitized solar cell.
出处
《物理学报》
SCIE
EI
CAS
CSCD
北大核心
2012年第9期51-57,共7页
Acta Physica Sinica
基金
国家自然科学基金(批准号:20973050)资助的课题~~